EN 10088-1 X1NiCrMoCu31-27-4 vs ASTM A240/A240M N08028

Strong Match — 85% match based on chemical composition and mechanical property overlap.

EN 10088-1 X1NiCrMoCu31-27-4 (EN 10088-1:2023) and ASTM A240/A240M N08028 (ASTM A240/A240M:2025) are both steel grades. Both fall under the Stainless Steel category. EN 10088-1 X1NiCrMoCu31-27-4 is defined under European Standard (EN), originating from Europe, while ASTM A240/A240M N08028 is defined under ASTM International, originating from United States.

As per chemical composition, EN 10088-1 X1NiCrMoCu31-27-4 vs ASTM A240/A240M N08028 is a 85% match. Mechanical property data is not available for both grades, so this factor could not be scored. Combined, this makes them a strong match overall at 85%.

Frequently Compared With EN 10088-1 X1NiCrMoCu31-27-4:
IS 1570 (Part 7) 12Cr12MoH IS 1570 (Part 7) 12Cr12Ni2Mo ASTM A959 26-3-3 ASTM A959 .- GB/T 3280 06Cr19Ni10 GOST 5632 06Kh23N28 GOST 5632 08X18H10 EN 10088-1 1.4006 EN 10088-1 1.4301 EN 10088-1 1.4401 EN 10088-1 1.4845 IS 1570 (Part 7) 11Cr17Ni13W3TiH
Match Breakdown
CHEMISTRY MATCH
85%
MECHANICAL MATCH
No shared data
OVERALL
85%
Specifications
Property EN 10088-1 X1NiCrMoCu31-27-4 ASTM A240/A240M N08028
Standard EN 10088-1:2023 ASTM A240/A240M:2025
Category Stainless Steel Stainless Steel
C (%) <=0.020 <=0.030
Si (%) <=0.70 <=1.00
Mn (%) <=2.00 <=2.50
P (%) <=0.030 <=0.030
S (%) <=0.010 <=0.030
Cr (%) 26.0-28.0 26.0-28.0
Mo (%) 3.00-4.0 3.0-4.0
Ni (%) 30.0-32.0 30.0-34.0
N (%) <=0.10 Not specified
Cu (%) 0.70-1.50 0.6-1.4
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property EN 10088-1 X1NiCrMoCu31-27-4 ASTM A240/A240M N08028
Tensile Strength Not specified >=500 MPa
Yield Strength Not specified >=214 MPa
Elongation Not specified >=40%
Hardness Not specified <=90 HRBW
Condition Not specified Plate, sheet and strip; yield by 0.2 percent offset
Typical Applications
EN 10088-1 X1NiCrMoCu31-27-4
Not documented
ASTM A240/A240M N08028
Pressure vessels and general applications (plate, sheet and strip)
Key Differences
Can EN 10088-1 X1NiCrMoCu31-27-4 Be Substituted With ASTM A240/A240M N08028?
EN 10088-1 X1NiCrMoCu31-27-4 and ASTM A240/A240M N08028 overlap closely enough on chemistry and mechanical properties that ASTM A240/A240M N08028 is often considered as a substitute for EN 10088-1 X1NiCrMoCu31-27-4 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.
On M-EX Right Now
EN 10088-1 X1NiCrMoCu31-27-4
0 active listings and RFQs →
ASTM A240/A240M N08028
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between EN 10088-1 X1NiCrMoCu31-27-4 and ASTM A240/A240M N08028?
EN 10088-1 X1NiCrMoCu31-27-4 specifies N which is not specified for ASTM A240/A240M N08028.
Can EN 10088-1 X1NiCrMoCu31-27-4 be substituted with ASTM A240/A240M N08028?
EN 10088-1 X1NiCrMoCu31-27-4 and ASTM A240/A240M N08028 overlap closely enough on chemistry and mechanical properties that ASTM A240/A240M N08028 is often considered as a substitute for EN 10088-1 X1NiCrMoCu31-27-4 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.