EN 10088-1 X1NiCrMoCuN25-20-7 vs ASTM A959 N08926

Strong Match — 98.1% match based on chemical composition and mechanical property overlap.

EN 10088-1 X1NiCrMoCuN25-20-7 (EN 10088-1:2023) and ASTM A959 N08926 (ASTM A959:2011) are both steel grades. Both fall under the Stainless Steel category. EN 10088-1 X1NiCrMoCuN25-20-7 is defined under European Standard (EN), originating from Europe, while ASTM A959 N08926 is defined under ASTM International, originating from United States.

As per chemical composition, EN 10088-1 X1NiCrMoCuN25-20-7 vs ASTM A959 N08926 is a 98.1% match. Mechanical property data is not available for both grades, so this factor could not be scored. Combined, this makes them a strong match overall at 98.1%.

Frequently Compared With EN 10088-1 X1NiCrMoCuN25-20-7:
IS 1570 (Part 7) 12Cr12MoVH ASTM A959 .- GB/T 3280 06Cr19Ni10 GOST 5632 06Kh23N28 GOST 5632 08X18H10 EN 10088-1 1.4006 EN 10088-1 1.4301 EN 10088-1 1.4401 EN 10088-1 1.4845 IS 1570 (Part 7) 11Cr17Ni13W3TiH IS 1570 (Part 7) 12Cr12MoH IS 1570 (Part 7) 12Cr12Ni2Mo
Match Breakdown
CHEMISTRY MATCH
98.1%
MECHANICAL MATCH
No shared data
OVERALL
98.1%
Specifications
Property EN 10088-1 X1NiCrMoCuN25-20-7 ASTM A959 N08926
Standard EN 10088-1:2023 ASTM A959:2011
Category Stainless Steel Stainless Steel
C (%) <=0.020 <=0.020
Si (%) <=0.75 <=0.50
Mn (%) <=2.00 <=2.00
P (%) <=0.030 <=0.030
S (%) <=0.010 <=0.010
Cr (%) 19.0-21.0 19.0-21.0
Mo (%) 6.0-7.0 6.0-7.0
Ni (%) 24.0-26.0 24.0-26.0
N (%) 0.15-0.25 0.15-0.25
Cu (%) 0.50-1.50 0.50-1.50
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Typical Applications
EN 10088-1 X1NiCrMoCuN25-20-7
Not documented
ASTM A959 N08926
Wrought stainless steel products; recommended composition limits for adoption by product standards (clause 1.1)
Can EN 10088-1 X1NiCrMoCuN25-20-7 Be Substituted With ASTM A959 N08926?
EN 10088-1 X1NiCrMoCuN25-20-7 and ASTM A959 N08926 overlap closely enough on chemistry and mechanical properties that ASTM A959 N08926 is often considered as a substitute for EN 10088-1 X1NiCrMoCuN25-20-7 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.
On M-EX Right Now
EN 10088-1 X1NiCrMoCuN25-20-7
0 active listings and RFQs →
ASTM A959 N08926
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between EN 10088-1 X1NiCrMoCuN25-20-7 and ASTM A959 N08926?
Both grades share a similar composition profile; see the specification table above for the exact chemistry and mechanical property values.
Can EN 10088-1 X1NiCrMoCuN25-20-7 be substituted with ASTM A959 N08926?
EN 10088-1 X1NiCrMoCuN25-20-7 and ASTM A959 N08926 overlap closely enough on chemistry and mechanical properties that ASTM A959 N08926 is often considered as a substitute for EN 10088-1 X1NiCrMoCuN25-20-7 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.