EN 10088-1 X2CrMnNiTi12 vs GOST 5632 06Kh23N28

Related Material — 63.9% match based on chemical composition and mechanical property overlap.

EN 10088-1 X2CrMnNiTi12 (EN 10088-1:2023) and GOST 5632 06Kh23N28 (GOST 5632-2014) are both steel grades. Both fall under the Stainless Steel category. EN 10088-1 X2CrMnNiTi12 is defined under European Standard (EN) (Europe).

As per chemical composition, EN 10088-1 X2CrMnNiTi12 vs GOST 5632 06Kh23N28 is a 63.9% match. Mechanical property data is not available for both grades, so this factor could not be scored. Combined, this makes them a related material overall at 63.9%.

Frequently Compared With EN 10088-1 X2CrMnNiTi12:
ASTM A959 .- GB/T 3280 06Cr19Ni10 EN 10088-1 1.4006 EN 10088-1 1.4301 EN 10088-1 1.4401 EN 10088-1 1.4845 IS 1570 (Part 7) 12Cr12MoVH GOST 5632 08X18H10 IS 1570 (Part 7) 11Cr17Ni13W3TiH IS 1570 (Part 7) 12Cr12MoH IS 1570 (Part 7) 12Cr12Ni2Mo IS 1570 (Part 7) 12Cr13H
Match Breakdown
CHEMISTRY MATCH
63.9%
MECHANICAL MATCH
No shared data
OVERALL
63.9%
Specifications
Property EN 10088-1 X2CrMnNiTi12 GOST 5632 06Kh23N28
Standard EN 10088-1:2023 GOST 5632-2014
Category Stainless Steel Stainless Steel
C (%) <=0.030 ≤0.06
Si (%) <=1.00 ≤0.80
Mn (%) 1.00-2.50 ≤2.00
P (%) <=0.040 Not specified
S (%) <=0.015 Not specified
Cr (%) 11.0-13.0 22.0–25.0
Ni (%) 0.30-1.00 26.0–29.0
N (%) <=0.025 Not specified
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property EN 10088-1 X2CrMnNiTi12 GOST 5632 06Kh23N28
Tensile Strength Not specified ≥510 MPa
Yield Strength Not specified ≥196 MPa
Elongation Not specified ≥35%
Max Service Temp Not specified 1050°C
Typical Applications
EN 10088-1 X2CrMnNiTi12
Not documented
GOST 5632 06Kh23N28
Furnace components, heat exchangers, high temperature applications
Key Differences
Can EN 10088-1 X2CrMnNiTi12 Be Substituted With GOST 5632 06Kh23N28?
EN 10088-1 X2CrMnNiTi12 and GOST 5632 06Kh23N28 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.
Forms & Sizes Available on M-EX
EN 10088-1 X2CrMnNiTi12
No active listings currently.
GOST 5632 06Kh23N28
Sheet → (2 listings)
Thickness: 6–6 mm (0.24–0.24 in)
Width: 1250–1250 mm (49.21–49.21 in)
Length: 3100–3400 mm (122.05–133.86 in)
On M-EX Right Now
EN 10088-1 X2CrMnNiTi12
0 active listings and RFQs →
GOST 5632 06Kh23N28
2 active listings and RFQs →
Frequently Asked Questions
What is the difference between EN 10088-1 X2CrMnNiTi12 and GOST 5632 06Kh23N28?
EN 10088-1 X2CrMnNiTi12 specifies P, S, N which are not specified for GOST 5632 06Kh23N28.
Can EN 10088-1 X2CrMnNiTi12 be substituted with GOST 5632 06Kh23N28?
EN 10088-1 X2CrMnNiTi12 and GOST 5632 06Kh23N28 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.