EN 10088-1 X6CrNi17-1 vs BS 970 (Part 1) 430S17

Close Alternative — 84.9% match based on chemical composition and mechanical property overlap.

EN 10088-1 X6CrNi17-1 (EN 10088-1:2023) and BS 970 (Part 1) 430S17 (BS 970 (Part 1):1991) are both steel grades. Both fall under the Stainless Steel category. EN 10088-1 X6CrNi17-1 is defined under European Standard (EN), originating from Europe, while BS 970 (Part 1) 430S17 is defined under British Standards (BS), originating from United Kingdom.

As per chemical composition, EN 10088-1 X6CrNi17-1 vs BS 970 (Part 1) 430S17 is a 90.3% match. Mechanical property data is not available for both grades, so this factor could not be scored. Combined, this makes them a close alternative overall at 84.9%.

Frequently Compared With EN 10088-1 X6CrNi17-1:
EN 10088-1 1.4006 EN 10088-1 1.4301 ASTM A959 .- GB/T 3280 06Cr19Ni10 GOST 5632 06Kh23N28 GOST 5632 08X18H10 EN 10088-1 1.4401 EN 10088-1 1.4845 IS 1570 (Part 7) 11Cr17Ni13W3TiH IS 1570 (Part 7) 12Cr12MoH IS 1570 (Part 7) 12Cr12MoVH IS 1570 (Part 7) 12Cr12Ni2Mo
Match Breakdown
CHEMISTRY MATCH
90.3%
MECHANICAL MATCH
No shared data
OVERALL
84.9%
Specifications
Property EN 10088-1 X6CrNi17-1 BS 970 (Part 1) 430S17
Standard EN 10088-1:2023 BS 970 (Part 1):1991
Category Stainless Steel Stainless Steel
C (%) <=0.08 <=0.08
Si (%) <=1.00 <=1.0
Mn (%) <=1.00 <=1.0
P (%) <=0.040 <=0.040
S (%) <=0.015 <=0.030
Cr (%) 16.0-18.0 16.0-18.0
Ni (%) 1.20-1.60 <=0.50
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Typical Applications
EN 10088-1 X6CrNi17-1
Not documented
BS 970 (Part 1) 430S17
Ferritic and martensitic stainless and heat resisting steel (section five)
Can EN 10088-1 X6CrNi17-1 Be Substituted With BS 970 (Part 1) 430S17?
EN 10088-1 X6CrNi17-1 and BS 970 (Part 1) 430S17 are a close alternative rather than a direct substitute. Some properties overlap well, but check the specific chemistry and mechanical rows above against your application's requirements before treating them as interchangeable.
On M-EX Right Now
EN 10088-1 X6CrNi17-1
0 active listings and RFQs →
BS 970 (Part 1) 430S17
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between EN 10088-1 X6CrNi17-1 and BS 970 (Part 1) 430S17?
Both grades share a similar composition profile; see the specification table above for the exact chemistry and mechanical property values.
Can EN 10088-1 X6CrNi17-1 be substituted with BS 970 (Part 1) 430S17?
EN 10088-1 X6CrNi17-1 and BS 970 (Part 1) 430S17 are a close alternative rather than a direct substitute. Some properties overlap well, but check the specific chemistry and mechanical rows above against your application's requirements before treating them as interchangeable.