EN 10088-1 X6CrNiTi12 vs ASTM A240/A240M S41008

Close Alternative — 76.2% match based on chemical composition and mechanical property overlap.

EN 10088-1 X6CrNiTi12 (EN 10088-1:2023) and ASTM A240/A240M S41008 (ASTM A240/A240M:2025) are both steel grades. Both fall under the Stainless Steel category. EN 10088-1 X6CrNiTi12 is defined under European Standard (EN), originating from Europe, while ASTM A240/A240M S41008 is defined under ASTM International, originating from United States.

As per chemical composition, EN 10088-1 X6CrNiTi12 vs ASTM A240/A240M S41008 is a 76.2% match. Mechanical property data is not available for both grades, so this factor could not be scored. Combined, this makes them a close alternative overall at 76.2%.

Frequently Compared With EN 10088-1 X6CrNiTi12:
EN 10088-1 1.4845 ASTM A959 .- GB/T 3280 06Cr19Ni10 GOST 5632 06Kh23N28 GOST 5632 08X18H10 EN 10088-1 1.4006 EN 10088-1 1.4301 EN 10088-1 1.4401 IS 1570 (Part 7) 11Cr17Ni13W3TiH IS 1570 (Part 7) 12Cr12MoH IS 1570 (Part 7) 12Cr12MoVH IS 1570 (Part 7) 12Cr12Ni2Mo
Match Breakdown
CHEMISTRY MATCH
76.2%
MECHANICAL MATCH
No shared data
OVERALL
76.2%
Specifications
Property EN 10088-1 X6CrNiTi12 ASTM A240/A240M S41008
Standard EN 10088-1:2023 ASTM A240/A240M:2025
Category Stainless Steel Stainless Steel
C (%) <=0.08 <=0.08
Si (%) <=0.70 <=1.00
Mn (%) <=1.50 <=1.00
P (%) <=0.040 <=0.040
S (%) <=0.015 <=0.030
Cr (%) 10.5-12.5 11.5-13.5
Ni (%) 0.50-1.50 <=0.60
Ti (%) 0.05-0.35 Not specified
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property EN 10088-1 X6CrNiTi12 ASTM A240/A240M S41008
Tensile Strength Not specified >=415 MPa
Yield Strength Not specified >=205 MPa
Elongation Not specified >=22%
Hardness Not specified <=183 HB
Condition Not specified Plate, sheet and strip; yield by 0.2 percent offset
Typical Applications
EN 10088-1 X6CrNiTi12
Not documented
ASTM A240/A240M S41008
Pressure vessels and general applications (plate, sheet and strip)
Key Differences
Can EN 10088-1 X6CrNiTi12 Be Substituted With ASTM A240/A240M S41008?
EN 10088-1 X6CrNiTi12 and ASTM A240/A240M S41008 are a close alternative rather than a direct substitute. Some properties overlap well, but check the specific chemistry and mechanical rows above against your application's requirements before treating them as interchangeable.
On M-EX Right Now
EN 10088-1 X6CrNiTi12
0 active listings and RFQs →
ASTM A240/A240M S41008
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between EN 10088-1 X6CrNiTi12 and ASTM A240/A240M S41008?
EN 10088-1 X6CrNiTi12 specifies Ti which is not specified for ASTM A240/A240M S41008.
Can EN 10088-1 X6CrNiTi12 be substituted with ASTM A240/A240M S41008?
EN 10088-1 X6CrNiTi12 and ASTM A240/A240M S41008 are a close alternative rather than a direct substitute. Some properties overlap well, but check the specific chemistry and mechanical rows above against your application's requirements before treating them as interchangeable.