EN 10088-2 X2CrMnNiN21-5-1 vs ASTM A240/A240M S32101

Close Alternative — 74.8% match based on chemical composition and mechanical property overlap.

EN 10088-2 X2CrMnNiN21-5-1 (EN 10088-2:2014) and ASTM A240/A240M S32101 (ASTM A240/A240M:2025) are both steel grades. Both fall under the Stainless Steel category. EN 10088-2 X2CrMnNiN21-5-1 is typically used for general purposes, hot or cold rolled sheet/plate and strip, while ASTM A240/A240M S32101 is commonly used for pressure vessels and general applications (plate, sheet and strip). EN 10088-2 X2CrMnNiN21-5-1 is defined under European Standard (EN), originating from Europe, while ASTM A240/A240M S32101 is defined under ASTM International, originating from United States.

As per chemical composition, EN 10088-2 X2CrMnNiN21-5-1 vs ASTM A240/A240M S32101 is a 95.6% match. As per mechanical properties, the match is 33.3%. Combined, this makes them a close alternative overall at 74.8%.

Frequently Compared With EN 10088-2 X2CrMnNiN21-5-1:
GOST 5632 06Kh23N28 EN 10088-1 1.4006 EN 10088-1 1.4301 EN 10088-1 1.4401 IS 1570 (Part 7) 12Cr12MoVH ASTM A959 .- GB/T 3280 06Cr19Ni10 GOST 5632 08X18H10 EN 10088-1 1.4845 IS 1570 (Part 7) 11Cr17Ni13W3TiH IS 1570 (Part 7) 12Cr12MoH IS 1570 (Part 7) 12Cr12Ni2Mo
Match Breakdown
CHEMISTRY MATCH
95.6%
MECHANICAL MATCH
33.3%
OVERALL
74.8%
Specifications
Property EN 10088-2 X2CrMnNiN21-5-1 ASTM A240/A240M S32101
Standard EN 10088-2:2014 ASTM A240/A240M:2025
Category Stainless Steel Stainless Steel
C (%) <=0.04 <=0.040
Si (%) <=1.00 <=1.00
Mn (%) 4.0-6.0 4.00-6.00
P (%) <=0.040 <=0.040
S (%) <=0.015 <=0.030
Cr (%) 21.0-22.0 21.0-22.0
Mo (%) 0.10-0.80 0.10-0.80
Ni (%) 1.35-1.90 1.35-1.70
N (%) 0.20-0.25 0.20-0.25
Cu (%) 0.10-0.80 0.10-0.80
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property EN 10088-2 X2CrMnNiN21-5-1 ASTM A240/A240M S32101
Tensile Strength 700-900 MPa >=700 MPa
Yield Strength >=530 MPa >=530 MPa
Elongation >=20% >=30%
Condition Solution annealed (+AT), cold rolled strip, up to 6.4 mm thick; Yield Strength is Rp0.2 (transverse), Elongation is A80 for under 3 mm thick t <= 0.187 in. [5.00 mm] (first condition printed); yield by 0.2 percent offset
Hardness Not specified <=290 HB
Typical Applications
EN 10088-2 X2CrMnNiN21-5-1
General purposes, hot or cold rolled sheet/plate and strip
ASTM A240/A240M S32101
Pressure vessels and general applications (plate, sheet and strip)
Can EN 10088-2 X2CrMnNiN21-5-1 Be Substituted With ASTM A240/A240M S32101?
EN 10088-2 X2CrMnNiN21-5-1 and ASTM A240/A240M S32101 are a close alternative rather than a direct substitute. Some properties overlap well, but check the specific chemistry and mechanical rows above against your application's requirements before treating them as interchangeable.
On M-EX Right Now
EN 10088-2 X2CrMnNiN21-5-1
0 active listings and RFQs →
ASTM A240/A240M S32101
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between EN 10088-2 X2CrMnNiN21-5-1 and ASTM A240/A240M S32101?
Both grades share a similar composition profile; see the specification table above for the exact chemistry and mechanical property values.
Can EN 10088-2 X2CrMnNiN21-5-1 be substituted with ASTM A240/A240M S32101?
EN 10088-2 X2CrMnNiN21-5-1 and ASTM A240/A240M S32101 are a close alternative rather than a direct substitute. Some properties overlap well, but check the specific chemistry and mechanical rows above against your application's requirements before treating them as interchangeable.