EN 10088-2 X2CrNiMoN17-13-5 vs EN 10088-1 X2CrNiMoN18-12-4

Close Alternative — 81.8% match based on chemical composition and mechanical property overlap.

EN 10088-2 X2CrNiMoN17-13-5 (EN 10088-2:2014) and EN 10088-1 X2CrNiMoN18-12-4 (EN 10088-1:2023) are both steel grades. Both fall under the Stainless Steel category. EN 10088-2 X2CrNiMoN17-13-5 is defined under European Standard (EN), originating from Europe, while EN 10088-1 X2CrNiMoN18-12-4 is defined under European Standard (EN), originating from Europe.

As per chemical composition, EN 10088-2 X2CrNiMoN17-13-5 vs EN 10088-1 X2CrNiMoN18-12-4 is a 81.8% match. Mechanical property data is not available for both grades, so this factor could not be scored. Combined, this makes them a close alternative overall at 81.8%.

Frequently Compared With EN 10088-2 X2CrNiMoN17-13-5:
GB/T 3280 06Cr19Ni10 IS 1570 (Part 7) 11Cr17Ni13W3TiH IS 1570 (Part 7) 12Cr12MoVH ASTM A959 .- GOST 5632 06Kh23N28 GOST 5632 08X18H10 EN 10088-1 1.4006 EN 10088-1 1.4301 EN 10088-1 1.4401 EN 10088-1 1.4845 IS 1570 (Part 7) 12Cr12MoH IS 1570 (Part 7) 12Cr12Ni2Mo
Match Breakdown
CHEMISTRY MATCH
81.8%
MECHANICAL MATCH
No shared data
OVERALL
81.8%
Specifications
Property EN 10088-2 X2CrNiMoN17-13-5 EN 10088-1 X2CrNiMoN18-12-4
Standard EN 10088-2:2014 EN 10088-1:2023
Category Stainless Steel Stainless Steel
C (%) <=0.030 <=0.030
Si (%) <=1.00 <=1.00
Mn (%) <=2.00 <=2.00
P (%) <=0.045 <=0.045
S (%) <=0.015 <=0.015
Cr (%) 16.5-18.5 16.5-19.5
Mo (%) 4.0-5.0 3.00-4.0
Ni (%) 12.5-14.5 10.5-14.0
N (%) 0.12-0.22 0.10-0.20
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property EN 10088-2 X2CrNiMoN17-13-5 EN 10088-1 X2CrNiMoN18-12-4
Tensile Strength 580-780 MPa Not specified
Yield Strength >=290 MPa Not specified
Elongation >=35% Not specified
Condition Solution annealed (+AT), cold rolled strip, up to 8 mm thick; Yield Strength is Rp0.2 (transverse), Elongation is A80 for under 3 mm thick Not specified
Typical Applications
EN 10088-2 X2CrNiMoN17-13-5
General purposes, hot or cold rolled sheet/plate and strip
EN 10088-1 X2CrNiMoN18-12-4
Not documented
Can EN 10088-2 X2CrNiMoN17-13-5 Be Substituted With EN 10088-1 X2CrNiMoN18-12-4?
EN 10088-2 X2CrNiMoN17-13-5 and EN 10088-1 X2CrNiMoN18-12-4 are a close alternative rather than a direct substitute. Some properties overlap well, but check the specific chemistry and mechanical rows above against your application's requirements before treating them as interchangeable.
On M-EX Right Now
EN 10088-2 X2CrNiMoN17-13-5
0 active listings and RFQs →
EN 10088-1 X2CrNiMoN18-12-4
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between EN 10088-2 X2CrNiMoN17-13-5 and EN 10088-1 X2CrNiMoN18-12-4?
Both grades share a similar composition profile; see the specification table above for the exact chemistry and mechanical property values.
Can EN 10088-2 X2CrNiMoN17-13-5 be substituted with EN 10088-1 X2CrNiMoN18-12-4?
EN 10088-2 X2CrNiMoN17-13-5 and EN 10088-1 X2CrNiMoN18-12-4 are a close alternative rather than a direct substitute. Some properties overlap well, but check the specific chemistry and mechanical rows above against your application's requirements before treating them as interchangeable.