EN 10088-2 X2CrNiN18-10 vs EN 10088-1 X2CrNiN18-10

Strong Match — 100% match based on chemical composition and mechanical property overlap.

EN 10088-2 X2CrNiN18-10 (EN 10088-2:2014) and EN 10088-1 X2CrNiN18-10 (EN 10088-1:2023) are both steel grades. Both fall under the Stainless Steel category. EN 10088-2 X2CrNiN18-10 is defined under European Standard (EN), originating from Europe, while EN 10088-1 X2CrNiN18-10 is defined under European Standard (EN), originating from Europe.

As per chemical composition, EN 10088-2 X2CrNiN18-10 vs EN 10088-1 X2CrNiN18-10 is a 100% match. Mechanical property data is not available for both grades, so this factor could not be scored. Combined, this makes them a strong match overall at 100%.

Frequently Compared With EN 10088-2 X2CrNiN18-10:
EN 10088-1 1.4006 EN 10088-1 1.4301 EN 10088-1 1.4401 EN 10088-1 1.4845 IS 1570 (Part 7) 12Cr12MoH IS 1570 (Part 7) 12Cr12MoVH IS 1570 (Part 7) 12Cr12Ni2Mo IS 1570 (Part 7) 12Cr13H ASTM A959 .- GB/T 3280 06Cr19Ni10 GOST 5632 06Kh23N28 GOST 5632 08X18H10
Match Breakdown
CHEMISTRY MATCH
100%
MECHANICAL MATCH
No shared data
OVERALL
100%
Specifications
Property EN 10088-2 X2CrNiN18-10 EN 10088-1 X2CrNiN18-10
Standard EN 10088-2:2014 EN 10088-1:2023
Category Stainless Steel Stainless Steel
C (%) <=0.030 <=0.030
Si (%) <=1.00 <=1.00
Mn (%) <=2.00 <=2.00
P (%) <=0.045 <=0.045
S (%) <=0.015 <=0.015
Cr (%) 17.5-19.5 17.5-19.5
Ni (%) 8.5-11.5 8.5-11.5
N (%) 0.12-0.22 0.12-0.22
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property EN 10088-2 X2CrNiN18-10 EN 10088-1 X2CrNiN18-10
Tensile Strength 550-750 MPa Not specified
Yield Strength >=290 MPa Not specified
Elongation >=40% Not specified
Condition Solution annealed (+AT), cold rolled strip, up to 8 mm thick; Yield Strength is Rp0.2 (transverse), Elongation is A80 for under 3 mm thick Not specified
Typical Applications
EN 10088-2 X2CrNiN18-10
General purposes, hot or cold rolled sheet/plate and strip
EN 10088-1 X2CrNiN18-10
Not documented
Can EN 10088-2 X2CrNiN18-10 Be Substituted With EN 10088-1 X2CrNiN18-10?
EN 10088-2 X2CrNiN18-10 and EN 10088-1 X2CrNiN18-10 overlap closely enough on chemistry and mechanical properties that EN 10088-1 X2CrNiN18-10 is often considered as a substitute for EN 10088-2 X2CrNiN18-10 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.
On M-EX Right Now
EN 10088-2 X2CrNiN18-10
0 active listings and RFQs →
EN 10088-1 X2CrNiN18-10
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between EN 10088-2 X2CrNiN18-10 and EN 10088-1 X2CrNiN18-10?
Both grades share a similar composition profile; see the specification table above for the exact chemistry and mechanical property values.
Can EN 10088-2 X2CrNiN18-10 be substituted with EN 10088-1 X2CrNiN18-10?
EN 10088-2 X2CrNiN18-10 and EN 10088-1 X2CrNiN18-10 overlap closely enough on chemistry and mechanical properties that EN 10088-1 X2CrNiN18-10 is often considered as a substitute for EN 10088-2 X2CrNiN18-10 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.