EN 10088-2 X4CrNiMo16-5-1 vs GB/T 3280 06Cr19Ni10

Minimal Match — 35% match based on chemical composition and mechanical property overlap.

EN 10088-2 X4CrNiMo16-5-1 (EN 10088-2:2014) and GB/T 3280 06Cr19Ni10 (GB/T 3280-2015) are both steel grades. Both fall under the Stainless Steel category. EN 10088-2 X4CrNiMo16-5-1 is typically used for general purposes, hot or cold rolled sheet/plate and strip, while GB/T 3280 06Cr19Ni10 is commonly used for used for kitchen equipment, food processing machinery, chemical tanks, piping, architectural panels, and fasteners.. EN 10088-2 X4CrNiMo16-5-1 is defined under European Standard (EN), originating from Europe, while GB/T 3280 06Cr19Ni10 is defined under Guobiao Standards (GB/T), originating from China.

As per chemical composition, EN 10088-2 X4CrNiMo16-5-1 vs GB/T 3280 06Cr19Ni10 is a 62.6% match. As per mechanical properties, the match is 0%. Combined, this makes them a minimal match overall at 35%.

Frequently Compared With EN 10088-2 X4CrNiMo16-5-1:
GOST 5632 06Kh23N28 EN 10088-1 1.4006 EN 10088-1 1.4301 EN 10088-1 1.4401 IS 1570 (Part 7) 12Cr12MoVH ASTM A959 .- GOST 5632 08X18H10 EN 10088-1 1.4845 IS 1570 (Part 7) 11Cr17Ni13W3TiH IS 1570 (Part 7) 12Cr12MoH IS 1570 (Part 7) 12Cr13H IS 1570 (Part 7) 12Cr12Ni2Mo
Match Breakdown
CHEMISTRY MATCH
62.6%
MECHANICAL MATCH
0%
OVERALL
35%
Specifications
Property EN 10088-2 X4CrNiMo16-5-1 GB/T 3280 06Cr19Ni10
Standard EN 10088-2:2014 GB/T 3280-2015
Category Stainless Steel Stainless Steel
C (%) <=0.06 0.08 max
Si (%) <=0.70 1.00 max
Mn (%) <=1.50 2.00 max
P (%) <=0.040 0.045 max
S (%) <=0.015 0.030 max
Cr (%) 15.0-17.0 18.00-20.00
Mo (%) 0.80-1.50 Not specified
Ni (%) 4.0-6.0 8.00-11.00
N (%) >=0.020 Not specified
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property EN 10088-2 X4CrNiMo16-5-1 GB/T 3280 06Cr19Ni10
Tensile Strength 840-1100 MPa 520-720 MPa
Yield Strength >=660 MPa 205-310 MPa
Elongation >=14% 40-60%
Condition Quenched and tempered (+QT840), hot rolled plate, up to 75 mm thick Not specified
Hardness Not specified 187 HB max
Typical Applications
EN 10088-2 X4CrNiMo16-5-1
General purposes, hot or cold rolled sheet/plate and strip
GB/T 3280 06Cr19Ni10
Used for kitchen equipment, food processing machinery, chemical tanks, piping, architectural panels, and fasteners.
Key Differences
Can EN 10088-2 X4CrNiMo16-5-1 Be Substituted With GB/T 3280 06Cr19Ni10?
EN 10088-2 X4CrNiMo16-5-1 and GB/T 3280 06Cr19Ni10 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.
Forms & Sizes Available on M-EX
EN 10088-2 X4CrNiMo16-5-1
No active listings currently.
GB/T 3280 06Cr19Ni10
Sheet → (2 listings)
Thickness: 6–6 mm (0.24–0.24 in)
Width: 1250–1250 mm (49.21–49.21 in)
Length: 2900–3300 mm (114.17–129.92 in)
On M-EX Right Now
EN 10088-2 X4CrNiMo16-5-1
0 active listings and RFQs →
GB/T 3280 06Cr19Ni10
2 active listings and RFQs →
Frequently Asked Questions
What is the difference between EN 10088-2 X4CrNiMo16-5-1 and GB/T 3280 06Cr19Ni10?
EN 10088-2 X4CrNiMo16-5-1 specifies Mo, N which are not specified for GB/T 3280 06Cr19Ni10.
Can EN 10088-2 X4CrNiMo16-5-1 be substituted with GB/T 3280 06Cr19Ni10?
EN 10088-2 X4CrNiMo16-5-1 and GB/T 3280 06Cr19Ni10 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.