EN 10088-3 X53CrSiMoVN16-2 vs EN 10088-1 1.4401

Minimal Match — 33.2% match based on chemical composition and mechanical property overlap.

EN 10088-3 X53CrSiMoVN16-2 (EN 10088-3:2014) and EN 10088-1 1.4401 (EN 10088-1:2014) are both steel grades. Both fall under the Stainless Steel category. EN 10088-3 X53CrSiMoVN16-2 is typically used for general purposes, semi-finished products, bars, rods, wire, sections and bright products, while EN 10088-1 1.4401 is commonly used for marine, chemical processing, pharmaceutical equipment. EN 10088-3 X53CrSiMoVN16-2 is defined under European Standard (EN), originating from Europe, while EN 10088-1 1.4401 is defined under European Standard (EN), originating from Europe.

As per chemical composition, EN 10088-3 X53CrSiMoVN16-2 vs EN 10088-1 1.4401 is a 49.8% match. As per mechanical properties, the match is 0%. Combined, this makes them a minimal match overall at 33.2%.

Frequently Compared With EN 10088-3 X53CrSiMoVN16-2:
EN 10088-1 1.4301 GB/T 3280 06Cr19Ni10 EN 10088-1 1.4845 IS 1570 (Part 7) 11Cr17Ni13W3TiH IS 1570 (Part 7) 12Cr12MoVH ASTM A959 .- GOST 5632 06Kh23N28 GOST 5632 08X18H10 EN 10088-1 1.4006 IS 1570 (Part 7) 12Cr12MoH IS 1570 (Part 7) 12Cr12Ni2Mo IS 1570 (Part 7) 12Cr13H
Match Breakdown
CHEMISTRY MATCH
49.8%
MECHANICAL MATCH
0%
OVERALL
33.2%
Specifications
Property EN 10088-3 X53CrSiMoVN16-2 EN 10088-1 1.4401
Standard EN 10088-3:2014 EN 10088-1:2014
Category Stainless Steel Stainless Steel
Si (%) 1.30-1.70 ≤1.00
Mn (%) <=0.80 ≤2.00
P (%) <=0.030 Not specified
S (%) <=0.010 Not specified
Cr (%) 15.0-16.5 16.5–18.5
Mo (%) 0.20-0.40 2.0–2.5
Ni (%) <=0.40 10.5–13.5
V (%) 0.20-0.40 Not specified
N (%) 0.05-0.20 Not specified
C (%) Not specified ≤0.07
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property EN 10088-3 X53CrSiMoVN16-2 EN 10088-1 1.4401
Hardness <=255 HB ≤215 HB
Condition Annealed (+A), conditions 1C, 1E, 1D, 1X, 1G and 2D, thickness or diameter up to 100 mm; hardness for guidance only Not specified
Tensile Strength Not specified ≥520 MPa
Yield Strength Not specified ≥210 MPa
Elongation Not specified ≥40%
Typical Applications
EN 10088-3 X53CrSiMoVN16-2
General purposes, semi-finished products, bars, rods, wire, sections and bright products
EN 10088-1 1.4401
Marine, chemical processing, pharmaceutical equipment
Key Differences
Can EN 10088-3 X53CrSiMoVN16-2 Be Substituted With EN 10088-1 1.4401?
EN 10088-3 X53CrSiMoVN16-2 and EN 10088-1 1.4401 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.
Forms & Sizes Available on M-EX
EN 10088-3 X53CrSiMoVN16-2
No active listings currently.
EN 10088-1 1.4401
Sheet → (4 listings)
Thickness: 6–6 mm (0.24–0.24 in)
Width: 1250–1250 mm (49.21–49.21 in)
Length: 2500–3400 mm (98.43–133.86 in)
On M-EX Right Now
EN 10088-3 X53CrSiMoVN16-2
0 active listings and RFQs →
EN 10088-1 1.4401
4 active listings and RFQs →
Frequently Asked Questions
What is the difference between EN 10088-3 X53CrSiMoVN16-2 and EN 10088-1 1.4401?
EN 10088-3 X53CrSiMoVN16-2 specifies P, S, V, N which are not specified for EN 10088-1 1.4401. EN 10088-1 1.4401 specifies C which is not specified for EN 10088-3 X53CrSiMoVN16-2.
Can EN 10088-3 X53CrSiMoVN16-2 be substituted with EN 10088-1 1.4401?
EN 10088-3 X53CrSiMoVN16-2 and EN 10088-1 1.4401 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.