EN 10088-3 X5CrNiCuNb16-4 vs EN 10088-1 X5CrNiCuNb16-4

Strong Match — 93.7% match based on chemical composition and mechanical property overlap.

EN 10088-3 X5CrNiCuNb16-4 (EN 10088-3:2014) and EN 10088-1 X5CrNiCuNb16-4 (EN 10088-1:2014) are both steel grades. Both fall under the Stainless Steel category. EN 10088-3 X5CrNiCuNb16-4 is defined under European Standard (EN), originating from Europe, while EN 10088-1 X5CrNiCuNb16-4 is defined under European Standard (EN), originating from Europe.

As per chemical composition, EN 10088-3 X5CrNiCuNb16-4 vs EN 10088-1 X5CrNiCuNb16-4 is a 93.7% match. Mechanical property data is not available for both grades, so this factor could not be scored. Combined, this makes them a strong match overall at 93.7%.

Frequently Compared With EN 10088-3 X5CrNiCuNb16-4:
GB/T 3280 06Cr19Ni10 GOST 5632 08X18H10 IS 1570 (Part 7) 11Cr17Ni13W3TiH IS 1570 (Part 7) 12Cr12MoH IS 1570 (Part 7) 12Cr12Ni2Mo ASTM A959 .- GOST 5632 06Kh23N28 EN 10088-1 1.4006 EN 10088-1 1.4301 EN 10088-1 1.4401 EN 10088-1 1.4845 IS 1570 (Part 7) 12Cr12MoVH
Match Breakdown
CHEMISTRY MATCH
93.7%
MECHANICAL MATCH
No shared data
OVERALL
93.7%
Specifications
Property EN 10088-3 X5CrNiCuNb16-4 EN 10088-1 X5CrNiCuNb16-4
Standard EN 10088-3:2014 EN 10088-1:2014
Category Stainless Steel Stainless Steel
C (%) <=0.07 <=0.07
Si (%) <=0.70 <=0.70
Mn (%) <=1.50 <=1.50
P (%) <=0.040 <=0.040
S (%) <=0.030 <=0.015
Cr (%) 15.0-17.0 15.0-17.0
Mo (%) <=0.60 <=0.60
Ni (%) 3.0-5.0 3.0-5.0
Cu (%) 3.0-5.0 3.0-5.0
Nb (%) <=0.45 Not specified
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property EN 10088-3 X5CrNiCuNb16-4 EN 10088-1 X5CrNiCuNb16-4
Tensile Strength <=1200 MPa Not specified
Hardness <=360 HB Not specified
Condition Solution annealed (+AT), conditions 1C, 1E, 1D, 1X, 1G and 2D, thickness or diameter up to 100 mm; hardness for guidance only Not specified
Typical Applications
EN 10088-3 X5CrNiCuNb16-4
General purposes, semi-finished products, bars, rods, wire, sections and bright products
EN 10088-1 X5CrNiCuNb16-4
Not documented
Key Differences
Can EN 10088-3 X5CrNiCuNb16-4 Be Substituted With EN 10088-1 X5CrNiCuNb16-4?
EN 10088-3 X5CrNiCuNb16-4 and EN 10088-1 X5CrNiCuNb16-4 overlap closely enough on chemistry and mechanical properties that EN 10088-1 X5CrNiCuNb16-4 is often considered as a substitute for EN 10088-3 X5CrNiCuNb16-4 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.
On M-EX Right Now
EN 10088-3 X5CrNiCuNb16-4
0 active listings and RFQs →
EN 10088-1 X5CrNiCuNb16-4
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between EN 10088-3 X5CrNiCuNb16-4 and EN 10088-1 X5CrNiCuNb16-4?
EN 10088-3 X5CrNiCuNb16-4 specifies Nb which is not specified for EN 10088-1 X5CrNiCuNb16-4.
Can EN 10088-3 X5CrNiCuNb16-4 be substituted with EN 10088-1 X5CrNiCuNb16-4?
EN 10088-3 X5CrNiCuNb16-4 and EN 10088-1 X5CrNiCuNb16-4 overlap closely enough on chemistry and mechanical properties that EN 10088-1 X5CrNiCuNb16-4 is often considered as a substitute for EN 10088-3 X5CrNiCuNb16-4 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.