Minimal Match — 35% match
based on chemical composition and mechanical property overlap.
GB/T 1591 Q355C (GB/T 1591:2018) and ASTM A1008 SS Grade 50 (ASTM A1008) are both steel grades.
Both fall under the Structural Steel category.
GB/T 1591 Q355C is typically used for general structure for engineering (plates, strips, bars and sections), while ASTM A1008 SS Grade 50 is commonly used for cold-rolled high-strength structural steel sheet; automotive structural components, cold-formed parts requiring moderate strength.
GB/T 1591 Q355C is defined under Guobiao Standards (GB/T), originating from China, while ASTM A1008 SS Grade 50 is defined under ASTM International, originating from United States.
As per chemical composition, GB/T 1591 Q355C vs ASTM A1008 SS Grade 50 is a 78.2% match.
As per mechanical properties, the match is 0%.
Combined, this makes them a minimal match overall at 35%.
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property
GB/T 1591 Q355C
ASTM A1008 SS Grade 50
Tensile Strength
470-630 MPa
380 MPa min
Yield Strength
>=355 MPa
340 MPa min
Elongation
>=22%
14% min
Condition
Hot-rolled (as-rolled), nominal thickness or diameter up to 16 mm for yield; tensile strength for up to 100 mm; elongation longitudinal, up to 40 mm
Not specified
Typical Applications
GB/T 1591 Q355C
General structure for engineering (plates, strips, bars and sections)
GB/T 1591 Q355C specifies Cr, Ni, Cu, N which are not specified for ASTM A1008 SS Grade 50.
Can GB/T 1591 Q355C Be Substituted With ASTM A1008 SS Grade 50?
GB/T 1591 Q355C and ASTM A1008 SS Grade 50 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.
What is the difference between GB/T 1591 Q355C and ASTM A1008 SS Grade 50?
GB/T 1591 Q355C specifies Cr, Ni, Cu, N which are not specified for ASTM A1008 SS Grade 50.