GB/T 3077 40MnVB vs GB/T 3077 25MnB

Close Alternative — 72.9% match based on chemical composition and mechanical property overlap.

GB/T 3077 40MnVB (GB/T 3077:2015) and GB/T 3077 25MnB (GB/T 3077:2015) are both steel grades. Both fall under the Alloy Steel category. GB/T 3077 40MnVB is typically used for hot-rolled or forged structural alloy steel bars, while GB/T 3077 25MnB is commonly used for hot-rolled or forged structural alloy steel bars. GB/T 3077 40MnVB is defined under Guobiao Standards (GB/T), originating from China, while GB/T 3077 25MnB is defined under Guobiao Standards (GB/T), originating from China.

As per chemical composition, GB/T 3077 40MnVB vs GB/T 3077 25MnB is a 84.3% match. As per mechanical properties, the match is 50%. Combined, this makes them a close alternative overall at 72.9%.

Frequently Compared With GB/T 3077 40MnVB:
NF A35-565 100C6 IS 1570 (Part 4) 103Cr6 IS 1570 (Part 7) 10Cr36Mo10H IS 1570 (Part 4) 07Cr4Mo6 UNI 11234 100Cr6 IS 1570 (Part 4) 103Cr4 IS 1570 (Part 4) 105Cr5 IS 4367 10Cr9Mo10 IS 1570 (Part 4) 10Mo6 IS 1570 (Part 7) 10Mo6H IS 4367 07Cr4Mo6 IS 1570 (Part 4) 10Cr20Mo6
Match Breakdown
CHEMISTRY MATCH
84.3%
MECHANICAL MATCH
50%
OVERALL
72.9%
Specifications
Property GB/T 3077 40MnVB GB/T 3077 25MnB
Standard GB/T 3077:2015 GB/T 3077:2015
Category Alloy Steel Alloy Steel
C (%) 0.37-0.44 0.23-0.28
Si (%) 0.17-0.37 0.17-0.37
Mn (%) 1.10-1.40 1.00-1.40
B (%) 0.0008-0.0035 0.0008-0.0035
V (%) 0.05-0.10 Not specified
P (%) <=0.030 <=0.030
S (%) <=0.030 <=0.030
Cu (%) <=0.30 <=0.30
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property GB/T 3077 40MnVB GB/T 3077 25MnB
Tensile Strength >=980 MPa >=835 MPa
Yield Strength >=785 MPa >=635 MPa
Elongation >=10% >=10%
Hardness <=207 HB <=207 HB
Condition Quenched and tempered, test sample 25 mm; hardness is for bars delivered annealed or high temperature tempered Quenched and tempered, test sample 25 mm; hardness is for bars delivered annealed or high temperature tempered
Typical Applications
GB/T 3077 40MnVB
Hot-rolled or forged structural alloy steel bars
GB/T 3077 25MnB
Hot-rolled or forged structural alloy steel bars
Key Differences
Can GB/T 3077 40MnVB Be Substituted With GB/T 3077 25MnB?
GB/T 3077 40MnVB and GB/T 3077 25MnB are a close alternative rather than a direct substitute. Some properties overlap well, but check the specific chemistry and mechanical rows above against your application's requirements before treating them as interchangeable.
On M-EX Right Now
GB/T 3077 40MnVB
0 active listings and RFQs →
GB/T 3077 25MnB
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between GB/T 3077 40MnVB and GB/T 3077 25MnB?
GB/T 3077 40MnVB specifies V which is not specified for GB/T 3077 25MnB.
Can GB/T 3077 40MnVB be substituted with GB/T 3077 25MnB?
GB/T 3077 40MnVB and GB/T 3077 25MnB are a close alternative rather than a direct substitute. Some properties overlap well, but check the specific chemistry and mechanical rows above against your application's requirements before treating them as interchangeable.