Close Alternative — 80.9% match
based on chemical composition and mechanical property overlap.
GB/T 3077 50Cr (GB/T 3077:2015) and IS 1570 (Part 4) 50Cr4V2 (IS 1570 (Part 4):1988) are both steel grades.
Both fall under the Alloy Steel category.
GB/T 3077 50Cr is defined under Guobiao Standards (GB/T), originating from China, while IS 1570 (Part 4) 50Cr4V2 is defined under Bureau of Indian Standards (IS), originating from India.
As per chemical composition, GB/T 3077 50Cr vs IS 1570 (Part 4) 50Cr4V2 is a 80.9% match.
Mechanical property data is not available for both grades, so this factor could not be scored.
Combined, this makes them a close alternative overall at 80.9%.
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property
GB/T 3077 50Cr
IS 1570 (Part 4) 50Cr4V2
Tensile Strength
>=1080 MPa
Not specified
Yield Strength
>=930 MPa
Not specified
Elongation
>=9%
Not specified
Hardness
<=229 HB
Not specified
Condition
Quenched and tempered, test sample 25 mm; hardness is for bars delivered annealed or high temperature tempered
Not specified
Typical Applications
GB/T 3077 50Cr
Hot-rolled or forged structural alloy steel bars
IS 1570 (Part 4) 50Cr4V2
Not documented
Key Differences
GB/T 3077 50Cr specifies P, S, Cu which are not specified for IS 1570 (Part 4) 50Cr4V2.
IS 1570 (Part 4) 50Cr4V2 specifies V which is not specified for GB/T 3077 50Cr.
Can GB/T 3077 50Cr Be Substituted With IS 1570 (Part 4) 50Cr4V2?
GB/T 3077 50Cr and IS 1570 (Part 4) 50Cr4V2 are a close alternative rather than a direct substitute. Some properties overlap well, but check the specific chemistry and mechanical rows above against your application's requirements before treating them as interchangeable.
What is the difference between GB/T 3077 50Cr and IS 1570 (Part 4) 50Cr4V2?
GB/T 3077 50Cr specifies P, S, Cu which are not specified for IS 1570 (Part 4) 50Cr4V2. IS 1570 (Part 4) 50Cr4V2 specifies V which is not specified for GB/T 3077 50Cr.
Can GB/T 3077 50Cr be substituted with IS 1570 (Part 4) 50Cr4V2?
GB/T 3077 50Cr and IS 1570 (Part 4) 50Cr4V2 are a close alternative rather than a direct substitute. Some properties overlap well, but check the specific chemistry and mechanical rows above against your application's requirements before treating them as interchangeable.