IS 11169 (Part 1) 41Cr3 vs GB/T 3077 40CrNiMo

Close Alternative — 71.1% match based on chemical composition and mechanical property overlap.

IS 11169 (Part 1) 41Cr3 (IS 11169 (Part 1):2022) and GB/T 3077 40CrNiMo (GB/T 3077:2015) are both steel grades. Both fall under the Alloy Steel category. IS 11169 (Part 1) 41Cr3 is typically used for cold heading and cold extrusion of parts that are quenched and tempered; the standard covers bars, wire rods and wires of 2 to 100 mm (clause 1.1, annex c), while GB/T 3077 40CrNiMo is commonly used for hot-rolled or forged structural alloy steel bars. IS 11169 (Part 1) 41Cr3 is defined under Bureau of Indian Standards (IS), originating from India, while GB/T 3077 40CrNiMo is defined under Guobiao Standards (GB/T), originating from China.

As per chemical composition, IS 11169 (Part 1) 41Cr3 vs GB/T 3077 40CrNiMo is a 71.1% match. Mechanical property data is not available for both grades, so this factor could not be scored. Combined, this makes them a close alternative overall at 71.1%.

Frequently Compared With IS 11169 (Part 1) 41Cr3:
NF A35-565 100C6 IS 4367 07Cr4Mo6 IS 1570 (Part 7) 10Cr36Mo10H IS 1570 (Part 4) 07Cr4Mo6 IS 1570 (Part 4) 103Cr6 IS 1570 (Part 7) 10Mo6H IS 11169 (Part 1) 10Ni5Cr4 UNI 11234 100Cr6 IS 1570 (Part 4) 103Cr4 IS 1570 (Part 4) 105Cr5 IS 1570 (Part 4) 10Cr20Mo6 IS 4367 10Cr9Mo10
Match Breakdown
CHEMISTRY MATCH
71.1%
MECHANICAL MATCH
No shared data
OVERALL
71.1%
Specifications
Property IS 11169 (Part 1) 41Cr3 GB/T 3077 40CrNiMo
Standard IS 11169 (Part 1):2022 GB/T 3077:2015
Category Alloy Steel Alloy Steel
C (%) 0.38-0.43 0.37-0.44
Cr (%) 0.70-0.90 0.60-0.90
Cu (%) <=0.35 <=0.30
Mn (%) 0.70-0.90 0.50-0.80
Mo (%) <=0.06 0.15-0.25
Ni (%) <=0.25 1.25-1.65
P (%) <=0.030 <=0.030
S (%) <=0.040 <=0.030
Si (%) 0.15-0.35 0.17-0.37
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property IS 11169 (Part 1) 41Cr3 GB/T 3077 40CrNiMo
Tensile Strength Not specified >=980 MPa
Yield Strength Not specified >=835 MPa
Elongation Not specified >=12%
Hardness Not specified <=269 HB
Condition Not specified Quenched and tempered, test sample 25 mm; hardness is for bars delivered annealed or high temperature tempered
Typical Applications
IS 11169 (Part 1) 41Cr3
Cold heading and cold extrusion of parts that are quenched and tempered; the standard covers bars, wire rods and wires of 2 to 100 mm (clause 1.1, Annex C)
GB/T 3077 40CrNiMo
Hot-rolled or forged structural alloy steel bars
Can IS 11169 (Part 1) 41Cr3 Be Substituted With GB/T 3077 40CrNiMo?
IS 11169 (Part 1) 41Cr3 and GB/T 3077 40CrNiMo are a close alternative rather than a direct substitute. Some properties overlap well, but check the specific chemistry and mechanical rows above against your application's requirements before treating them as interchangeable.
On M-EX Right Now
IS 11169 (Part 1) 41Cr3
0 active listings and RFQs →
GB/T 3077 40CrNiMo
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between IS 11169 (Part 1) 41Cr3 and GB/T 3077 40CrNiMo?
Both grades share a similar composition profile; see the specification table above for the exact chemistry and mechanical property values.
Can IS 11169 (Part 1) 41Cr3 be substituted with GB/T 3077 40CrNiMo?
IS 11169 (Part 1) 41Cr3 and GB/T 3077 40CrNiMo are a close alternative rather than a direct substitute. Some properties overlap well, but check the specific chemistry and mechanical rows above against your application's requirements before treating them as interchangeable.