IS 1570 (Part 7):1992 Fe360H Steel: Specifications & Listings

IS 1570 (Part 7):1992 Fe360H: Fe360H: steel for elevated temperature service (creep resisting steel). Specified in IS 1570 (Part 7):1992.

Category: Carbon Steel
Grade Details
GradeIS 1570 (Part 7):1992 Fe360H
Standard IS 1570 (Part 7):1992
ApplicationsBoilers, pressure vessels, steam turbines, steam and water piping and other power plant equipment working at elevated temperature
Grade ComparisonCompare With a Specific Grade →
Grade Standard Match
IS 1570 (Part 7) Fe410H IS 1570 (Part 7):1992 Close Alternative
IS 11169 (Part 1) 40C15 IS 11169 (Part 1):2022 Related Material
IS 1570 (Part 4) 10Mo6 IS 1570 (Part 4):1988 Related Material
IS 1570 (Part 4) 20Mo6 IS 1570 (Part 4):1988 Related Material
IS 1570 (Part 4) 33Mo6 IS 1570 (Part 4):1988 Related Material
IS 1570 (Part 4) 07Cr4Mo6 IS 1570 (Part 4):1988 Related Material
IS 1570 (Part 4) 10Cr20Mo6 IS 1570 (Part 4):1988 Related Material
IS 11169 (Part 1) 20Ni7Mo2 IS 11169 (Part 1):2022 Related Material
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Chemical Composition (%)
C Si Mn P S Cr Ni Mo Cu
<=0.20 0.10-0.35 0.40-1.20 <=0.03 <=0.03 <=0.25 <=0.30 <=0.10 <=0.30
Mechanical Properties
Tensile Strength 360-480 MPa
Yield Strength >=205 MPa (0.2 % proof stress)
Elongation >=26%
Condition Plate, N, thickness over 3 to 16 (first row of Table 3)

More data from IS 1570 (Part 7):1992

From the standard
Mechanical properties at room temperature 5 rows
ProductHeat treatmentThickness (mm)Hardness (RB)Rp0.2 min (MPa)Rm min (MPa)Rm max (MPa)Elongation min (%)KV (J)Bend test D max
PlateNover 3 to 16-20536048026-0.5a
PlateNover 16 to 40-19536048026-0.5a
PlateNover 40 to 63-18536048025-0.5a
PlateNover 63 to 100-17536048024-0.5a
PlateNover 100 to 150-17036048024-0.5a
Rm and elongation printed once for a group of thickness rows are repeated on each row; Rp0.2 'Note 8' is printed as in the standard; in case of dispute the tensile strength value is deciding.
Source: IS 1570 (Part 7):1992, Table 3
0.2 % proof stress at elevated temperature (guidance only) Rp0.2 min in MPa
Product, heat treatment, thickness150 deg C200 deg C250 deg C300 deg C350 deg C400 deg C
Plate, N, 3 to 16 mm172168150124117115
Plate, N, over 16 to 40 mm169162144124117115
Plate, N, over 40 to 63 mm158152141124117115
Plate, N, over 63 to 100 mm148144136124117115
For guidance only.
Source: IS 1570 (Part 7):1992, Table 4
Heat treatment 4 entries
Normalising temperature
900 to 930 deg C
Normalising time
1 to 2 min per 1 mm
Normalising cooling
in quiet air
Stress relief or tempering after bending or welding
600 to 650 deg C, 2 min per 1 mm
Indications are for guidance only except where test samples are reference heat treated; stress relief temperature should be at least 30 deg C below the tempering temperature.
Source: IS 1570 (Part 7):1992, Table 5

Active IS 1570 (Part 7):1992 Fe360H Listings on M-EX (For Sale)

+ Create a Listing for this grade

No active IS 1570 (Part 7):1992 Fe360H listings at this time.

Register for Alerts

Buyer RFQs for IS 1570 (Part 7):1992 Fe360H

+ Post an RFQ for this grade

No open buyer requirements for IS 1570 (Part 7):1992 Fe360H at this time.

Register for Alerts