IS 2062 E350 vs IS 2062 E350A

Strong Match — 100% match based on chemical composition and mechanical property overlap.

IS 2062 E350 (IS 2062:2006) and IS 2062 E350A (IS 2062:2009) are both steel grades. Both fall under the Structural Steel category. IS 2062 E350 is typically used for structural work: welded, bolted and riveted structures and general engineering purposes, while IS 2062 E350A is commonly used for structural work: welded, bolted and riveted structures and general engineering purposes. IS 2062 E350 is defined under Bureau of Indian Standards (IS), originating from India, while IS 2062 E350A is defined under Bureau of Indian Standards (IS), originating from India.

As per chemical composition, IS 2062 E350 vs IS 2062 E350A is a 100% match. As per mechanical properties, the match is 100%. Combined, this makes them a strong match overall at 100%.

Frequently Compared With IS 2062 E350:
GOST 19281 09G2S CSA G40.21 400W CSA G40.21 480W CSA G40.21 300W CSA G40.21 350W CSA G40.21 400A CSA G40.21 260W ASTM A1008 SS Grade 50 ASTM A1008 SS Grade 80 ASTM A572 Gr.65 AS/NZS 3679.1 350 ASTM A283C
Match Breakdown
CHEMISTRY MATCH
100%
MECHANICAL MATCH
100%
OVERALL
100%
Specifications
Property IS 2062 E350 IS 2062 E350A
Standard IS 2062:2006 IS 2062:2009
Category Structural Steel Structural Steel
C (%) <=0.20 <=0.20
Mn (%) <=1.50 <=1.50
S (%) <=0.045 <=0.045
P (%) <=0.045 <=0.045
Si (%) <=0.45 <=0.45
CEV (%) <=0.42 <=0.42
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property IS 2062 E350 IS 2062 E350A
Tensile Strength >=490 MPa >=490 MPa
Yield Strength 350 MPa (<20mm) / 330 MPa (20-40mm) / 320 MPa (>40mm) 350 MPa (<20mm) / 330 MPa (20-40mm) / 320 MPa (>40mm)
Elongation >=22% >=22%
Impact Energy >=50 J at room temperature (25 +/- 2°C) / >=25 J at -20°C Not specified
Impact Not specified not required
Typical Applications
IS 2062 E350
Structural work: welded, bolted and riveted structures and general engineering purposes
IS 2062 E350A
Structural work: welded, bolted and riveted structures and general engineering purposes
Can IS 2062 E350 Be Substituted With IS 2062 E350A?
IS 2062 E350 and IS 2062 E350A overlap closely enough on chemistry and mechanical properties that IS 2062 E350A is often considered as a substitute for IS 2062 E350 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.
On M-EX Right Now
IS 2062 E350
0 active listings and RFQs →
IS 2062 E350A
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between IS 2062 E350 and IS 2062 E350A?
Both grades share a similar composition profile; see the specification table above for the exact chemistry and mechanical property values.
Can IS 2062 E350 be substituted with IS 2062 E350A?
IS 2062 E350 and IS 2062 E350A overlap closely enough on chemistry and mechanical properties that IS 2062 E350A is often considered as a substitute for IS 2062 E350 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.