JIS G4304:2021 SUS317 Steel: Specifications & Listings

JIS G4304:2021 SUS317: SUS317: austenitic stainless steel, hot-rolled plate, sheet and strip. Specified in JIS G 4304:2021.

Category: Stainless Steel
Grade Details
GradeJIS G4304:2021 SUS317
Standard JIS G4304:2021
ApplicationsHot-rolled stainless steel plates and strips
Equivalent / Similar Grades
Grade Standard Region Live on M-EX
ASTM A959 317 ASTM A959:2011 USA No activity yet
ASTM A276/A276M S31700 ASTM A276/A276M:2017 USA No activity yet
IS 6603 X04Cr18Ni12Mo3 IS 6603:2024 India No activity yet
JIS G4305 SUS317 JIS G4305:2012 Japan No activity yet
JIS G4305 SUS316 JIS G4305:2012 Japan No activity yet
JIS G4305 SUS316Ti JIS G4305:2012 Japan No activity yet
Grade ComparisonCompare With a Specific Grade →
Grade Standard Match
ASTM A959 317 ASTM A959:2011 Strong Match
JIS G4305 SUS317 JIS G4305:2012 Strong Match
ASTM A276/A276M S31700 ASTM A276/A276M:2017 Strong Match
IS 6603 X04Cr18Ni12Mo3 IS 6603:2024 Strong Match
JIS G4304 SUS316 JIS G4304:2021 Strong Match
JIS G4304 SUS316Ti JIS G4304:2021 Strong Match
JIS G4305 SUS316 JIS G4305:2012 Strong Match
JIS G4305 SUS316Ti JIS G4305:2012 Strong Match
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Chemical Composition (%)
C Si Mn P S Ni Cr Mo
<=0.08 <=1.00 <=2.00 <=0.045 <=0.030 11.00-15.00 18.00-20.00 3.00-4.00
Mechanical Properties
Tensile Strength >=520 MPa
Yield Strength >=205 MPa
Elongation >=40%
Hardness <=187 HB
Condition Solution heat treated plate and strip; 0.2 percent proof strength applies only when specified by the purchaser

More data from JIS G4304:2021

From the standard
Mechanical properties, solution heat treated 3 values
0.2 percent proof strength, min
205 MPa
Tensile strength, min
520 MPa
Elongation, min
40 %
0.2 percent proof strength applies only when specified by the purchaser. 1 N/mm2 = 1 MPa.
Source: JIS G 4304:2021, Table 8
Hardness, solution heat treated 3 scales
Brinell hardness HBW, max
187
Rockwell HRBW or HRBS, max
90
Vickers hardness HV, max
200
Any one of the hardness scales applies; if not specified the manufacturer selects. HRBW is used in case of dispute.
Source: JIS G 4304:2021, Table 8
Heat treatment (example, informative) 1 settings
Solution heat treatment
1010 to 1150 deg C, rapid cooling
Annex JA is informative; temperatures are examples.
Source: JIS G 4304:2021, Table JA.1

Active JIS G4304:2021 SUS317 Listings on M-EX (For Sale)

+ Create a Listing for this grade

No active JIS G4304:2021 SUS317 listings at this time.

Register for Alerts

Buyer RFQs for JIS G4304:2021 SUS317

+ Post an RFQ for this grade

No open buyer requirements for JIS G4304:2021 SUS317 at this time.

Register for Alerts