JIS G4304 SUS347 vs JIS G4304 SUS321

Strong Match — 100% match based on chemical composition and mechanical property overlap.

JIS G4304 SUS347 (JIS G4304:2021) and JIS G4304 SUS321 (JIS G4304:2021) are both steel grades. Both fall under the Stainless Steel category. JIS G4304 SUS347 is typically used for hot-rolled stainless steel plates and strips, while JIS G4304 SUS321 is commonly used for hot-rolled stainless steel plates and strips. JIS G4304 SUS347 is defined under Japanese Industrial Standards (JIS), originating from Japan, while JIS G4304 SUS321 is defined under Japanese Industrial Standards (JIS), originating from Japan.

As per chemical composition, JIS G4304 SUS347 vs JIS G4304 SUS321 is a 100% match. As per mechanical properties, the match is 100%. Combined, this makes them a strong match overall at 100%.

Frequently Compared With JIS G4304 SUS347:
EN 10088-1 1.4845 ASTM A959 .- GB/T 3280 06Cr19Ni10 GOST 5632 06Kh23N28 GOST 5632 08X18H10 EN 10088-1 1.4006 EN 10088-1 1.4301 EN 10088-1 1.4401 IS 1570 (Part 7) 11Cr17Ni13W3TiH IS 1570 (Part 7) 12Cr12MoH IS 1570 (Part 7) 12Cr12MoVH IS 1570 (Part 7) 12Cr12Ni2Mo
Match Breakdown
CHEMISTRY MATCH
100%
MECHANICAL MATCH
100%
OVERALL
100%
Specifications
Property JIS G4304 SUS347 JIS G4304 SUS321
Standard JIS G4304:2021 JIS G4304:2021
Category Stainless Steel Stainless Steel
C (%) <=0.08 <=0.08
Si (%) <=1.00 <=1.00
Mn (%) <=2.00 <=2.00
P (%) <=0.045 <=0.045
S (%) <=0.030 <=0.030
Ni (%) 9.00-13.00 9.00-13.00
Cr (%) 17.00-19.00 17.00-19.00
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property JIS G4304 SUS347 JIS G4304 SUS321
Tensile Strength >=520 MPa >=520 MPa
Yield Strength >=205 MPa >=205 MPa
Elongation >=40% >=40%
Hardness <=187 HB <=187 HB
Condition Solution heat treated plate and strip; 0.2 percent proof strength applies only when specified by the purchaser Solution heat treated plate and strip; 0.2 percent proof strength applies only when specified by the purchaser
Typical Applications
JIS G4304 SUS347
Hot-rolled stainless steel plates and strips
JIS G4304 SUS321
Hot-rolled stainless steel plates and strips
Can JIS G4304 SUS347 Be Substituted With JIS G4304 SUS321?
JIS G4304 SUS347 and JIS G4304 SUS321 overlap closely enough on chemistry and mechanical properties that JIS G4304 SUS321 is often considered as a substitute for JIS G4304 SUS347 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.
On M-EX Right Now
JIS G4304 SUS347
0 active listings and RFQs →
JIS G4304 SUS321
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between JIS G4304 SUS347 and JIS G4304 SUS321?
Both grades share a similar composition profile; see the specification table above for the exact chemistry and mechanical property values.
Can JIS G4304 SUS347 be substituted with JIS G4304 SUS321?
JIS G4304 SUS347 and JIS G4304 SUS321 overlap closely enough on chemistry and mechanical properties that JIS G4304 SUS321 is often considered as a substitute for JIS G4304 SUS347 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.