JIS G4305:2012 SUS309S Steel: Specifications & Listings

JIS G4305:2012 SUS309S: SUS309S: austenitic stainless steel, cold-rolled plate, sheet and strip. Specified in JIS G 4305:2012.

Category: Stainless Steel
Grade Details
GradeJIS G4305:2012 SUS309S
Standard JIS G4305:2012
ApplicationsCold-rolled stainless steel plates, sheet and strip
Equivalent / Similar Grades
Grade Standard Region Live on M-EX
ASTM A959 309 ASTM A959:2011 USA No activity yet
ASTM A959 309S ASTM A959:2011 USA No activity yet
ASTM A959 309H ASTM A959:2011 USA No activity yet
ASTM A959 309Cb ASTM A959:2011 USA No activity yet
ASTM A959 309HCb ASTM A959:2011 USA No activity yet
EN 10088-1 X12CrNi23-13 EN 10088-1:2014 Europe (CEN) No activity yet
EN 10088-1 X6CrNi23-13 EN 10088-1:2014 Europe (CEN) No activity yet
JIS G4304 SUS309S JIS G4304:2021 Japan No activity yet
Grade ComparisonCompare With a Specific Grade →
Grade Standard Match
ASTM A959 309S ASTM A959:2011 Strong Match
JIS G4304 SUS309S JIS G4304:2021 Strong Match
ASTM A959 309Cb ASTM A959:2011 Strong Match
ASTM A959 309 ASTM A959:2011 Strong Match
ASTM A959 309H ASTM A959:2011 Strong Match
ASTM A959 309HCb ASTM A959:2011 Strong Match
EN 10088-1 X6CrNi23-13 EN 10088-1:2014 Strong Match
EN 10088-1 X6CrNi23-13 EN 10088-1:2023 Strong Match
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Chemical Composition (%)
C Si Mn P S Ni Cr
<=0.08 <=1.00 <=2.00 <=0.045 <=0.030 12.00-15.00 22.00-24.00
Mechanical Properties
Tensile Strength >=520 MPa
Yield Strength >=205 MPa
Elongation >=40%
Hardness <=187 HB
Condition Solution heat treated plate and strip; 0.2 percent proof strength applies only when specified by the purchaser

More data from JIS G4305:2012

From the standard
Mechanical properties, solution heat treated 3 values
0.2 percent proof strength, min
205 MPa
Tensile strength, min
520 MPa
Elongation, min
40 %
0.2 percent proof strength applies only when specified by the purchaser. 1 N/mm2 = 1 MPa.
Source: JIS G 4305:2012, Table 8
Hardness, solution heat treated 3 scales
Brinell hardness HBW, max
187
Rockwell HRBW or HRBS, max
90
Vickers hardness HV, max
200
Any one of the hardness scales applies; if not specified the manufacturer selects. HRBW is used in case of dispute.
Source: JIS G 4305:2012, Table 8
Heat treatment (example, informative) 1 settings
Solution heat treatment
1030 to 1180 deg C, rapid cooling
Annex JA is informative; temperatures are examples.
Source: JIS G 4305:2012, Table JA.1

Active JIS G4305:2012 SUS309S Listings on M-EX (For Sale)

+ Create a Listing for this grade

No active JIS G4305:2012 SUS309S listings at this time.

Register for Alerts

Buyer RFQs for JIS G4305:2012 SUS309S

+ Post an RFQ for this grade

No open buyer requirements for JIS G4305:2012 SUS309S at this time.

Register for Alerts