SAE J403:2001 1074 Steel: Specifications & Listings

SAE J403:2001 1074: Nonresulfurized carbon steel SAE 1074 (UNS G10740) to SAE J403 NOV2001, a chemistry-only grade for semifinished products for forging, hot rolled and cold finished bars, wire rods, plates, strip, sheets, welded tubing and seamless tubing. Carbon 0.70-0.80% and manganese 0.50-0.80%.

Category: Carbon Steel
Grade Details
GradeSAE J403:2001 1074
Standard SAE J403:2001
ApplicationsChemistry-only grade; product scope as listed in the composition notes
Equivalent / Similar Grades
Grade Standard Region Live on M-EX
IS 1570 (Part 2/Sec 1) 70C6 IS 1570 (Part 2/Sec 1):1979 India No activity yet
IS 1570 (Part 2/Sec 1) 75C6 IS 1570 (Part 2/Sec 1):1979 India No activity yet
SAE J403 1074 SAE J403:2009 USA No activity yet
DIN 17222 C75 DIN 17222:1979-08 Germany 3 listings, 0 RFQs →
IS 1570 (Part 2/Sec 1) 80C6 IS 1570 (Part 2/Sec 1):1979 India No activity yet
BS 970 (Part 1) 060A72 BS 970 (Part 1):1991 UK No activity yet
BS 970 (Part 1) 060A78 BS 970 (Part 1):1991 UK No activity yet
IS 1570 (Part 2/Sec 1) 60C6 IS 1570 (Part 2/Sec 1):1979 India No activity yet
IS 1570 (Part 2/Sec 1) 65C6 IS 1570 (Part 2/Sec 1):1979 India No activity yet
Grade ComparisonCompare With a Specific Grade →
Grade Standard Match
SAE J403 1074 SAE J403:2009 Strong Match
IS 1570 (Part 2/Sec 1) 75C6 IS 1570 (Part 2/Sec 1):1979 Strong Match
SAE J403 1074 SAE J403:2014 Strong Match
SAE J403 1075 SAE J403:2001 Strong Match
SAE J403 1075 SAE J403:2009 Strong Match
SAE J403 1075 SAE J403:2014 Strong Match
DIN 17222 C75 DIN 17222:1979-08 Strong Match
IS 1570 (Part 2/Sec 1) 70C6 IS 1570 (Part 2/Sec 1):1979 Strong Match
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Chemical Composition (%)
C Mn P S
0.70-0.80 0.50-0.80 <=0.030 <=0.050

More data from SAE J403:2001

From the standard
Other composition limits from the table and its notes
UNS number
G10740
Product scope
semifinished products for forging, hot rolled and cold finished bars, wire rods, plates, strip, sheets, welded tubing and seamless tubing
Silicon, when required, is commonly specified as 0.10% max or a range such as 0.15 to 0.35%. Lead (0.15 to 0.35%, letter L) and boron (0.0005 to 0.003%, letter B) versions of the standard grades are identified by a letter between the second and third digits.
Source: SAE J403:2001, Table 1, nonresulfurized carbon steels and its notes

Active SAE J403:2001 1074 Listings on M-EX (For Sale)

+ Create a Listing for this grade

No active SAE J403:2001 1074 listings at this time.

Register for Alerts

Buyer RFQs for SAE J403:2001 1074

+ Post an RFQ for this grade

No open buyer requirements for SAE J403:2001 1074 at this time.

Register for Alerts