SAE J403:2009 1002: Nonresulfurized carbon steel SAE 1002 (UNS G10020) to SAE J403 DEC2009, a chemistry-only grade for semifinished products for forging, hot rolled and cold finished bars, wire rods, plates, strip, sheets, welded tubing and seamless tubing. Carbon 0.02-0.04% and manganese up to 0.35%.

Category: Carbon Steel
Grade Details
GradeSAE J403:2009 1002
Standard SAE J403:2009
ApplicationsChemistry-only grade; product scope as listed in the composition notes
Equivalent / Similar Grades
Grade Standard Region Live on M-EX
IS 1570 (Part 2/Sec 1) 2C2 IS 1570 (Part 2/Sec 1):1979 India No activity yet
SAE J403 1002 SAE J403:2014 USA No activity yet
DIN 1654-2 C8C DIN 1654-2:1989-10 Germany 0 listings, 2 RFQs →
Grade ComparisonCompare With a Specific Grade →
Grade Standard Match
SAE J403 1002 SAE J403:2014 Strong Match
IS 1570 (Part 2/Sec 1) 2C2 IS 1570 (Part 2/Sec 1):1979 Strong Match
DIN 1654-2 C8C DIN 1654-2:1989-10 Strong Match
ASTM A36 ASTM A36 Close Alternative
ASTM A105 ASTM A105 Close Alternative
ASME SA105 ASME BPVC.II.A-2025 SA-105/SA-105M Close Alternative
GB/T 700 Q235 GB/T 700-2006 Related Material
EN 10025-2 E295 EN 10025-2:2019 Related Material
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Chemical Composition (%)
C Mn P S
0.02-0.04 <=0.35 <=0.030 <=0.050

More data from SAE J403:2009

From the standard
Other composition limits from the table and its notes
UNS number
G10020
Product scope
semifinished products for forging, hot rolled and cold finished bars, wire rods, plates, strip, sheets, welded tubing and seamless tubing
Residual limits, Option A
Cu 0.20, Ni 0.20, Cr 0.15, Mo 0.06 max
Residual limits, Option B (default)
Cu 0.35, Ni 0.25, Cr 0.20, Mo 0.06 max
Residual limits, Option C
Cu 0.40, Ni 0.40, Cr 0.30, Mo 0.12 max
Residual limits, Option D
No limits, values reported
Ultra low carbon, interstitial free stabilized and nonstabilized steel shall not be supplied for this grade. Silicon, when required, is commonly specified as 0.10% max or a range such as 0.15 to 0.35%. Lead (0.15 to 0.35%, letter L) and boron (0.0005 to 0.003%, letter B) versions of the standard grades are identified by a letter between the second and third digits. Residual elements are agreed between purchaser and supplier; unless otherwise specified Option B applies. Option A applies to flat rolled products up to 1060.
Source: SAE J403:2009, Table 1, nonresulfurized carbon steels and its notes

Active SAE J403:2009 1002 Listings on M-EX (For Sale)

+ Create a Listing for this grade

No active SAE J403:2009 1002 listings at this time.

Register for Alerts

Buyer RFQs for SAE J403:2009 1002

+ Post an RFQ for this grade

No open buyer requirements for SAE J403:2009 1002 at this time.

Register for Alerts