Market Intelligence  ›  Price Gap  ›  EN 10083-3 51CrV4

EN 10083-3 51CrV4 Steel: Price Gap

Demand price (median buyer ceiling from RFQs) versus offer price (median seller reserve from listings), and the gap between them, for EN 10083-3 51CrV4 across India. Click a region to drill into states.

Live Signal Lifetime
Live Signal: The gap between what buyers are bidding and what sellers are asking, from listings and RFQs open right now. Use this to price today. For example, “Are buyers currently bidding above what sellers ask for this grade?”
Viewing a specific grade. Switch grade:
Clear ×
Market direction
NA
Price gap (National)
NA
Current
NA
0 RFQs · 3 listings
7 days ago
NA
0 RFQs · 3 listings
15 days ago
NA
0 RFQs · 3 listings
30 days ago
NA
0 RFQs · 3 listings
Demand above offer (positive gap)
Offer above demand (negative gap)
Insufficient data (< 3 each side)
See activity (demand & supply) across India ›

Disclaimer: All information on this page is indicative only and derived from posted listings and RFQs on M-EX. It does not constitute a market price quote or investment advice. M-EX and GTE make no representations as to accuracy or completeness. Actual activity depends on quantity, quality, payment terms and other commercial factors agreed between buyers and sellers.

EN 10083-3 51CrV4 is a Spring Steel grade: A chromium vanadium alloy steel for quenching and tempering to EN 10083-3:2006 (steel number 1.8159). Supplied as semi-finished products, bars, rod, wide flats, hot rolled strip, sheet and plate, and forgings. Quenched and tempered tensile strength 1100 to 1300 MPa for ruling sections up to 16 mm. Typical applications: Valve springs, clutch springs, high duty coil springs.
Equivalent / Similar Grades (10)
Grade Standard Region
EN47 BS 970 UK
AISI 6150 SAE USA
SUP10 JIS Japan
SAE5160 SAE USA
ISO 51CrV4 ISO 683-1:1987 International
DIN 50CrV4 (1.8159) DIN Germany
BS 735A50 BS UK
NF 50CV 4 NF France
UNI 50CrV4 UNI Italy
UNE 51CrV4 (F1430) UNE Spain
Chemical Composition (%)
C Cr Mn P S Si V
0.47-0.55 0.90-1.20 0.70-1.10 <=0.025 <=0.025 <=0.40 0.10-0.25
Mechanical Properties
Condition Quenched and tempered (+QT), ruling section d <= 16 mm
Elongation 9% min
Hardness Soft annealed (+A): 248 HBW max
Tensile Strength 1100 to 1300 MPa
Yield Strength 900 MPa min