Market Intelligence  ›  Supply and Demand Balance  ›  EN 10083-2 C60

EN 10083-2 C60 Steel: Supply & Demand

Buyer RFQ demand against seller listing supply for EN 10083-2 C60, broken down by form. Signals are indicative and derived from listings and RFQs.

Last updated: 16 Oct 2026, 1:00 AM

Live Signal Lifetime
Lifetime: This grade’s supply and demand by form, across everything ever listed on M-EX. Use this for the long view. For example, “Has this grade historically drawn more buyers than sellers?”
Shortage
1
In Demand
0
Healthy
0
Oversupplied
0
Deep Supply
0
Low Activity
0
Form Supply Demand Status Price Band (Rs./MT)
Round Bar 0 33 Shortage 56,055 to 60,688
median 57,232
EN 10083-2 C60's demand ranks in the top 11% of all 484 tracked grades platform-wide.
The Round Bar form most recently moved into Shortage, 125 days ago.

Disclaimer: All information on this page is indicative only and derived from posted listings and RFQs on M-EX. It does not constitute a market price quote or investment advice. M-EX and GTE make no representations as to accuracy or completeness. Actual activity depends on quantity, quality, payment terms and other commercial factors agreed between buyers and sellers.

EN 10083-2 C60 is a Carbon Steel grade: A higher carbon steel for quenching and tempering to EN 10083-2:2006 (steel number 1.0601, non alloy quality steel). Supplied as semi-finished products, bars, rod, wide flats, hot rolled strip, sheet and plate, and forgings. Quenched and tempered tensile strength 850 to 1 000 MPa for ruling sections up to 16 mm. Typical applications: Used in springs, knives, wear plates, high-strength wires, and hand tools..
Equivalent / Similar Grades (4)
Grade Standard Region
SWRH62B JIS G3506 Japan
ISO C60 ISO 683-1:1987 International
DIN C 60 (1.0601) DIN Germany
UNI C60 UNI Italy
Chemical Composition (%)
C Cr Cr+Mo+Ni Mn Mo Ni P S Si
0.57-0.65 <=0.40 <=0.63 0.60-0.90 <=0.10 <=0.40 <=0.045 <=0.045 <=0.40
Mechanical Properties
Condition Quenched and tempered (+QT), ruling section d <= 16 mm
Elongation 11% min
Hardness Soft annealed (+A): 241 HBW max
Tensile Strength 850 to 1 000 MPa
Yield Strength 580 MPa min