AISI D2 KNL vs GB/T 1299 4Cr5MoSiV1

Minimal Match — 39.6% match based on chemical composition and mechanical property overlap.

AISI D2 KNL (ASTM A681) and GB/T 1299 4Cr5MoSiV1 (GB/T 1299-2014) are both steel grades. Both fall under the Tool & Die Steels category. AISI D2 KNL is typically used for blanking dies, forming dies, thread rolling dies, punches, shear blades, gauges, broaches, drawing dies, while GB/T 1299 4Cr5MoSiV1 is commonly used for die casting dies, forging dies, extrusion tools. AISI D2 KNL is defined under AISI, originating from United States, while GB/T 1299 4Cr5MoSiV1 is defined under Guobiao Standards (GB/T), originating from China.

As per chemical composition, AISI D2 KNL vs GB/T 1299 4Cr5MoSiV1 is a 59.5% match. As per mechanical properties, the match is 0%. Combined, this makes them a minimal match overall at 39.6%.

Frequently Compared With AISI D2 KNL:
DIN EN ISO 4957 1.2379 EN ISO 683-17 100Cr6 GB/T 1299 3Cr2W8V DIN EN ISO 4957 1.2344 EN ISO 4957 1.2316 GB/T 1299 4Cr5MoSiV GOST 5950 4H5MFS GOST 5950 3H2W8F GOST 5950 4H5MFS1 AISI 52100 IS 1570 (Part 6) 103T3 IS 3748 103T3
Match Breakdown
CHEMISTRY MATCH
59.5%
MECHANICAL MATCH
0%
OVERALL
39.6%
Specifications
Property AISI D2 KNL GB/T 1299 4Cr5MoSiV1
Standard ASTM A681 GB/T 1299-2014
Category Tool & Die Steels Tool & Die Steels
C (%) 1.40–1.60 0.32–0.45
Mn (%) ≤0.60 0.20–0.50
Si (%) ≤0.40 0.80–1.20
Cr (%) 11.00–13.00 4.75–5.50
Mo (%) 0.70–1.20 1.20–1.75
V (%) ≤1.00 0.80–1.20
S (%) ≤0.030 Not specified
P (%) ≤0.030 Not specified
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property AISI D2 KNL GB/T 1299 4Cr5MoSiV1
Hardness (annealed) ≤255 HB Not specified
Hardness (hardened) 58–62 HRC Not specified
Compressive Strength 2600 MPa Not specified
Hardness HRC (hardened) Not specified 42–54
Hardness HB (annealed) Not specified ≤235
Typical Applications
AISI D2 KNL
Blanking dies, forming dies, thread rolling dies, punches, shear blades, gauges, broaches, drawing dies
GB/T 1299 4Cr5MoSiV1
Die casting dies, forging dies, extrusion tools
Key Differences
Can AISI D2 KNL Be Substituted With GB/T 1299 4Cr5MoSiV1?
AISI D2 KNL and GB/T 1299 4Cr5MoSiV1 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.
Forms & Sizes Available on M-EX
AISI D2 KNL
Round Bar → (2 listings)
Diameter: 80–80 mm (3.15–3.15 in)
Length: 2500–3600 mm (98.43–141.73 in)
GB/T 1299 4Cr5MoSiV1
Round Bar → (2 listings)
Diameter: 80–80 mm (3.15–3.15 in)
Length: 2700–4100 mm (106.3–161.42 in)
On M-EX Right Now
AISI D2 KNL
2 active listings and RFQs →
GB/T 1299 4Cr5MoSiV1
2 active listings and RFQs →
Frequently Asked Questions
What is the difference between AISI D2 KNL and GB/T 1299 4Cr5MoSiV1?
AISI D2 KNL specifies S, P which are not specified for GB/T 1299 4Cr5MoSiV1.
Can AISI D2 KNL be substituted with GB/T 1299 4Cr5MoSiV1?
AISI D2 KNL and GB/T 1299 4Cr5MoSiV1 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.