ASTM A240/A240M S24000 vs ASTM A959 .-

Minimal Match — 35% match based on chemical composition and mechanical property overlap.

ASTM A240/A240M S24000 (ASTM A240/A240M:2025) and ASTM A959 .- (ASTM A959:2011) are both steel grades. Both fall under the Stainless Steel category. ASTM A240/A240M S24000 is typically used for pressure vessels and general applications (plate, sheet and strip), while ASTM A959 .- is commonly used for wrought stainless steel products; recommended composition limits for adoption by product standards (clause 1.1). ASTM A240/A240M S24000 is defined under ASTM International, originating from United States, while ASTM A959 .- is defined under ASTM International, originating from United States.

As per chemical composition, ASTM A240/A240M S24000 vs ASTM A959 .- is a 61.9% match. Mechanical property data is not available for both grades, so this factor could not be scored. Combined, this makes them a minimal match overall at 35%.

Frequently Compared With ASTM A240/A240M S24000:
GOST 5632 06Kh23N28 GOST 5632 08X18H10 EN 10088-1 1.4301 IS 1570 (Part 7) 12Cr12MoH IS 1570 (Part 7) 12Cr12Ni2Mo GB/T 3280 06Cr19Ni10 EN 10088-1 1.4006 EN 10088-1 1.4401 EN 10088-1 1.4845 IS 1570 (Part 7) 11Cr17Ni13W3TiH IS 1570 (Part 7) 12Cr12MoVH IS 1570 (Part 7) 12Cr13H
Match Breakdown
CHEMISTRY MATCH
61.9%
MECHANICAL MATCH
No shared data
OVERALL
35%
Specifications
Property ASTM A240/A240M S24000 ASTM A959 .-
Standard ASTM A240/A240M:2025 ASTM A959:2011
Category Stainless Steel Stainless Steel
C (%) <=0.08 <=0.030
Mn (%) 11.50-14.50 <=1.00
P (%) <=0.060 <=0.040
S (%) <=0.030 <=0.030
Si (%) <=0.75 <=1.00
Cr (%) 17.0-19.0 18.0-20.0
Ni (%) 2.3-3.7 <=0.50
N (%) 0.20-0.40 <=0.030
Cb (%) Not specified 0.10-0.60
Ti (%) Not specified 0.07-0.30
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property ASTM A240/A240M S24000 ASTM A959 .-
Tensile Strength >=690 MPa Not specified
Yield Strength >=415 MPa Not specified
Elongation >=40% Not specified
Hardness <=241 HB Not specified
Condition Sheet and strip (first condition printed); yield by 0.2 percent offset Not specified
Typical Applications
ASTM A240/A240M S24000
Pressure vessels and general applications (plate, sheet and strip)
ASTM A959 .-
Wrought stainless steel products; recommended composition limits for adoption by product standards (clause 1.1)
Key Differences
Can ASTM A240/A240M S24000 Be Substituted With ASTM A959 .-?
ASTM A240/A240M S24000 and ASTM A959 .- share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.
On M-EX Right Now
ASTM A240/A240M S24000
0 active listings and RFQs →
ASTM A959 .-
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between ASTM A240/A240M S24000 and ASTM A959 .-?
ASTM A959 .- specifies Cb, Ti which are not specified for ASTM A240/A240M S24000.
Can ASTM A240/A240M S24000 be substituted with ASTM A959 .-?
ASTM A240/A240M S24000 and ASTM A959 .- share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.