ASTM A959:2011 .- Steel: Specifications & Listings

ASTM A959:2011 .-: Ferritic stainless steel type .- (UNS S46800) with the composition limits of ASTM A959-11. Carbon up to 0.030% and chromium 18.0-20.0%.

Category: Stainless Steel
Grade Details
GradeASTM A959:2011 .-
Standard ASTM A959:2011
ApplicationsWrought stainless steel products; recommended composition limits for adoption by product standards (clause 1.1)
Equivalent / Similar Grades
Grade Standard Region Live on M-EX
ASTM A959 439 ASTM A959:2011 USA No activity yet
ASTM A959 S43932 ASTM A959:2011 USA No activity yet
ASTM A240/A240M S46800 ASTM A240/A240M:2025 USA No activity yet
ASTM A240/A240M S43035 ASTM A240/A240M:2025 USA No activity yet
JIS G4304 SUS430J1L JIS G4304:2021 Japan No activity yet
Grade ComparisonCompare With a Specific Grade →
Grade Standard Match
ASTM A240/A240M S46800 ASTM A240/A240M:2025 Strong Match
ASTM A240/A240M S43035 ASTM A240/A240M:2025 Strong Match
ASTM A959 439 ASTM A959:2011 Strong Match
ASTM A959 S43932 ASTM A959:2011 Strong Match
ASTM A240/A240M S43932 ASTM A240/A240M:2025 Strong Match
JIS G4304 SUS430J1L JIS G4304:2021 Strong Match
JIS G4305 SUS430J1L JIS G4305:2012 Strong Match
JIS G4304 SUS430LX JIS G4304:2021 Close Alternative
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Chemical Composition (%)
C Cb Cr Mn N Ni P S Si Ti
<=0.030 0.10-0.60 18.0-20.0 <=1.00 <=0.030 <=0.50 <=0.040 <=0.030 <=1.00 0.07-0.30

More data from ASTM A959:2011

From the standard
Other composition limits from Table 1 and its footnotes
UNS number
S46800
Metallurgical class
Ferritic grade: body-centered cubic, little or no tempered martensite, hardenable only slightly by cold working
Type
.- (designation originally assigned by the American Iron and Steel Institute)
Values
Maximum unless a range or minimum is shown; where two limits are shown for the same element in one grade the more stringent applies
Other elements (as printed)
Ti 0.07-0.30, Cb 0.10-0.60, and Ti+Cb 0.20+4x(C+N)-0.80
These are the recommended composition limits of the A959 guide, intended for adoption by standards for stainless steel products; they are not a product specification.
Source: ASTM A959:2011, Table 1 and its footnotes

Active ASTM A959:2011 .- Listings on M-EX (For Sale)

+ Create a Listing for this grade

No active ASTM A959:2011 .- listings at this time.