ASTM A240/A240M S31651 vs ASTM A276/A276M S31651

Strong Match — 88% match based on chemical composition and mechanical property overlap.

ASTM A240/A240M S31651 (ASTM A240/A240M:2025) and ASTM A276/A276M S31651 (ASTM A276/A276M:2017) are both steel grades. Both fall under the Stainless Steel category. ASTM A240/A240M S31651 is typically used for pressure vessels and general applications (plate, sheet and strip), while ASTM A276/A276M S31651 is commonly used for stainless steel bars and shapes (hot-finished or cold-finished). ASTM A240/A240M S31651 is defined under ASTM International, originating from United States, while ASTM A276/A276M S31651 is defined under ASTM International, originating from United States.

As per chemical composition, ASTM A240/A240M S31651 vs ASTM A276/A276M S31651 is a 98.6% match. As per mechanical properties, the match is 66.7%. Combined, this makes them a strong match overall at 88%.

Frequently Compared With ASTM A240/A240M S31651:
EN 10088-1 1.4845 EN 10088-1 1.4006 ASTM A959 .- GOST 5632 06Kh23N28 EN 10088-1 1.4401 GOST 5632 08X18H10 EN 10088-1 1.4301 IS 1570 (Part 7) 12Cr12MoH IS 1570 (Part 7) 12Cr12Ni2Mo GB/T 3280 06Cr19Ni10 IS 1570 (Part 7) 11Cr17Ni13W3TiH IS 1570 (Part 7) 12Cr12MoVH
Match Breakdown
CHEMISTRY MATCH
98.6%
MECHANICAL MATCH
66.7%
OVERALL
88%
Specifications
Property ASTM A240/A240M S31651 ASTM A276/A276M S31651
Standard ASTM A240/A240M:2025 ASTM A276/A276M:2017
Category Stainless Steel Stainless Steel
C (%) <=0.08 <=0.08
Mn (%) <=2.00 <=2.00
P (%) <=0.045 <=0.045
S (%) <=0.030 <=0.030
Si (%) <=0.75 <=1.00
Cr (%) 16.0-18.0 16.0-18.0
Ni (%) 10.0-14.0 10.0-14.0
Mo (%) 2.00-3.00 2.00-3.00
N (%) 0.10-0.16 0.10-0.16
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property ASTM A240/A240M S31651 ASTM A276/A276M S31651
Tensile Strength >=550 MPa >=550 MPa
Yield Strength >=240 MPa >=240 MPa
Elongation >=35% >=30%
Hardness <=217 HB Not specified
Condition Plate, sheet and strip; yield by 0.2 percent offset Condition A (Annealed), hot-finished or cold-finished, all sizes (first row printed)
Typical Applications
ASTM A240/A240M S31651
Pressure vessels and general applications (plate, sheet and strip)
ASTM A276/A276M S31651
Stainless steel bars and shapes (hot-finished or cold-finished)
Can ASTM A240/A240M S31651 Be Substituted With ASTM A276/A276M S31651?
ASTM A240/A240M S31651 and ASTM A276/A276M S31651 overlap closely enough on chemistry and mechanical properties that ASTM A276/A276M S31651 is often considered as a substitute for ASTM A240/A240M S31651 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.
On M-EX Right Now
ASTM A240/A240M S31651
0 active listings and RFQs →
ASTM A276/A276M S31651
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between ASTM A240/A240M S31651 and ASTM A276/A276M S31651?
Both grades share a similar composition profile; see the specification table above for the exact chemistry and mechanical property values.
Can ASTM A240/A240M S31651 be substituted with ASTM A276/A276M S31651?
ASTM A240/A240M S31651 and ASTM A276/A276M S31651 overlap closely enough on chemistry and mechanical properties that ASTM A276/A276M S31651 is often considered as a substitute for ASTM A240/A240M S31651 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.