ASTM A276/A276M S32750 vs JIS G4304 SUS327L1

Strong Match — 91.7% match based on chemical composition and mechanical property overlap.

ASTM A276/A276M S32750 (ASTM A276/A276M:2017) and JIS G4304 SUS327L1 (JIS G4304:2021) are both steel grades. Both fall under the Stainless Steel category. ASTM A276/A276M S32750 is typically used for stainless steel bars and shapes (hot-finished or cold-finished), while JIS G4304 SUS327L1 is commonly used for hot-rolled stainless steel plates and strips. ASTM A276/A276M S32750 is defined under ASTM International, originating from United States, while JIS G4304 SUS327L1 is defined under Japanese Industrial Standards (JIS), originating from Japan.

As per chemical composition, ASTM A276/A276M S32750 vs JIS G4304 SUS327L1 is a 100% match. As per mechanical properties, the match is 75%. Combined, this makes them a strong match overall at 91.7%.

Frequently Compared With ASTM A276/A276M S32750:
ASTM A959 2507 GOST 5632 06Kh23N28 EN 10088-1 1.4401 ASTM A959 .- EN 10088-1 1.4006 EN 10088-1 1.4301 EN 10088-1 1.4845 IS 1570 (Part 7) 11Cr17Ni13W3TiH GB/T 3280 06Cr19Ni10 GOST 5632 08X18H10 IS 1570 (Part 7) 12Cr12MoH IS 1570 (Part 7) 12Cr12MoVH
Match Breakdown
CHEMISTRY MATCH
100%
MECHANICAL MATCH
75%
OVERALL
91.7%
Specifications
Property ASTM A276/A276M S32750 JIS G4304 SUS327L1
Standard ASTM A276/A276M:2017 JIS G4304:2021
Category Stainless Steel Stainless Steel
C (%) <=0.030 <=0.030
Mn (%) <=1.20 <=1.20
P (%) <=0.035 <=0.035
S (%) <=0.020 <=0.020
Si (%) <=0.80 <=0.80
Cr (%) 24.0-26.0 24.00-26.00
Ni (%) 6.0-8.0 6.00-8.00
Mo (%) 3.0-5.0 3.00-5.00
N (%) 0.24-0.32 0.24-0.32
Cu (%) <=0.50 <=0.50
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property ASTM A276/A276M S32750 JIS G4304 SUS327L1
Tensile Strength >=800 MPa >=795 MPa
Yield Strength >=550 MPa >=550 MPa
Elongation >=15% >=15%
Hardness <=310 HB <=310 HB
Condition Condition A (Annealed), hot-finished or cold-finished, up to 2 [50.8] incl sizes (first row printed) Solution heat treated plate and strip; proof strength applies only when specified by the purchaser
Typical Applications
ASTM A276/A276M S32750
Stainless steel bars and shapes (hot-finished or cold-finished)
JIS G4304 SUS327L1
Hot-rolled stainless steel plates and strips
Can ASTM A276/A276M S32750 Be Substituted With JIS G4304 SUS327L1?
ASTM A276/A276M S32750 and JIS G4304 SUS327L1 overlap closely enough on chemistry and mechanical properties that JIS G4304 SUS327L1 is often considered as a substitute for ASTM A276/A276M S32750 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.
On M-EX Right Now
ASTM A276/A276M S32750
0 active listings and RFQs →
JIS G4304 SUS327L1
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between ASTM A276/A276M S32750 and JIS G4304 SUS327L1?
Both grades share a similar composition profile; see the specification table above for the exact chemistry and mechanical property values.
Can ASTM A276/A276M S32750 be substituted with JIS G4304 SUS327L1?
ASTM A276/A276M S32750 and JIS G4304 SUS327L1 overlap closely enough on chemistry and mechanical properties that JIS G4304 SUS327L1 is often considered as a substitute for ASTM A276/A276M S32750 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.