Related Material — 61% match
based on chemical composition and mechanical property overlap.
ASTM A36 (ASTM A36) and EN 10025-2 E360 (EN 10025-2:2019) are both steel grades.
ASTM A36 is classified under Carbon Steel, while EN 10025-2 E360 is classified under Structural Steel — a different category, which is worth noting alongside the chemistry match below.
ASTM A36 is typically used for structural fabrication, bridges, buildings, machinery parts, flanges, while EN 10025-2 E360 is commonly used for hot rolled products of structural steels.
ASTM A36 is defined under ASTM International, originating from United States, while EN 10025-2 E360 is defined under European Standard (EN), originating from Europe.
As per chemical composition, ASTM A36 vs EN 10025-2 E360 is a 91.5% match.
As per mechanical properties, the match is 0%.
Combined, this makes them a related material overall at 61%.
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property
ASTM A36
EN 10025-2 E360
Tensile Strength
400–550 MPa
670-830 MPa
Yield Strength
250 MPa min
>=360 MPa
Elongation
≥23%
>=11%
Condition
Not specified
Nominal thickness up to 16 mm (tensile for 3 to 100 mm, elongation for 3 to 40 mm), longitudinal test pieces
Different category: ASTM A36 is Carbon Steel, EN 10025-2 E360 is Structural Steel.
ASTM A36 specifies C, Mn, Si which are not specified for EN 10025-2 E360.
EN 10025-2 E360 specifies N which is not specified for ASTM A36.
Can ASTM A36 Be Substituted With EN 10025-2 E360?
ASTM A36 and EN 10025-2 E360 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.
What is the difference between ASTM A36 and EN 10025-2 E360?
Different category: ASTM A36 is Carbon Steel, EN 10025-2 E360 is Structural Steel. ASTM A36 specifies C, Mn, Si which are not specified for EN 10025-2 E360. EN 10025-2 E360 specifies N which is not specified for ASTM A36.
Can ASTM A36 be substituted with EN 10025-2 E360?
ASTM A36 and EN 10025-2 E360 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.