ASTM A959:2011 N08700: Austenitic stainless steel grade (UNS N08700) with the composition limits of ASTM A959-11. Carbon up to 0.04% and chromium 19.0-23.0%.
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Chemical Composition (%)
C
Cr
Cu
Mn
Mo
Ni
P
S
Si
<=0.04
19.0-23.0
<=0.50
<=2.00
4.3-5.0
24.0-26.0
<=0.040
<=0.030
<=1.00
More data from ASTM A959:2011
From the standard
Other composition limitsfrom Table 1 and its footnotes
UNS number
N08700
Metallurgical class
Austenitic grade: usually predominantly face-centered cubic, hardenable only by cold working
Type
No type number is printed; the grade is identified by its UNS number only
Values
Maximum unless a range or minimum is shown; where two limits are shown for the same element in one grade the more stringent applies
Other elements (as printed)
Cb 8xC min; 0.40 max
These are the recommended composition limits of the A959 guide, intended for adoption by standards for stainless steel products; they are not a product specification.
Source: ASTM A959:2011, Table 1 and its footnotes