ASTM A959:2011 S32654: Austenitic stainless steel grade (UNS S32654) with the composition limits of ASTM A959-11. Carbon up to 0.020% and chromium 24.0-25.0%.
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Chemical Composition (%)
C
Cr
Cu
Mn
Mo
N
Ni
P
S
Si
<=0.020
24.0-25.0
0.30-0.60
2.0-4.0
7.0-8.0
0.45-0.55
21.0-23.0
<=0.030
<=0.005
<=0.50
More data from ASTM A959:2011
From the standard
Other composition limitsfrom Table 1 and its footnotes
UNS number
S32654
Metallurgical class
Austenitic grade: usually predominantly face-centered cubic, hardenable only by cold working
Type
No type number is printed; the grade is identified by its UNS number only
Values
Maximum unless a range or minimum is shown; where two limits are shown for the same element in one grade the more stringent applies
Other elements (as printed)
Cu 0.30-0.60
These are the recommended composition limits of the A959 guide, intended for adoption by standards for stainless steel products; they are not a product specification.
Source: ASTM A959:2011, Table 1 and its footnotes