ASTM A959 S32760 vs ASTM A959 .-

Minimal Match — 35% match based on chemical composition and mechanical property overlap.

ASTM A959 S32760 (ASTM A959:2011) and ASTM A959 .- (ASTM A959:2011) are both steel grades. Both fall under the Stainless Steel category. ASTM A959 S32760 is typically used for wrought stainless steel products; recommended composition limits for adoption by product standards (clause 1.1), while ASTM A959 .- is commonly used for wrought stainless steel products; recommended composition limits for adoption by product standards (clause 1.1). ASTM A959 S32760 is defined under ASTM International, originating from United States, while ASTM A959 .- is defined under ASTM International, originating from United States.

As per chemical composition, ASTM A959 S32760 vs ASTM A959 .- is a 53% match. Mechanical property data is not available for both grades, so this factor could not be scored. Combined, this makes them a minimal match overall at 35%.

Frequently Compared With ASTM A959 S32760:
GB/T 3280 06Cr19Ni10 EN 10088-1 1.4301 ASTM A959 2507 EN 10088-1 1.4845 IS 1570 (Part 7) 11Cr17Ni13W3TiH EN 10088-1 1.4401 IS 1570 (Part 7) 12Cr12MoH ASTM A959 26-3-3 EN 10088-1 1.4006 IS 1570 (Part 7) 12Cr12MoVH IS 1570 (Part 7) 12Cr12Ni2Mo GOST 5632 08X18H10
Match Breakdown
CHEMISTRY MATCH
53%
MECHANICAL MATCH
No shared data
OVERALL
35%
Specifications
Property ASTM A959 S32760 ASTM A959 .-
Standard ASTM A959:2011 ASTM A959:2011
Category Stainless Steel Stainless Steel
C (%) <=0.030 <=0.030
Cr (%) 24.0-26.0 18.0-20.0
Cu (%) 0.50-1.00 Not specified
Mn (%) <=1.00 <=1.00
Mo (%) 3.0-4.0 Not specified
N (%) 0.20-0.30 <=0.030
Ni (%) 6.0-8.0 <=0.50
P (%) <=0.030 <=0.040
S (%) <=0.010 <=0.030
Si (%) <=1.00 <=1.00
W (%) 0.50-1.00 Not specified
Cb (%) Not specified 0.10-0.60
Ti (%) Not specified 0.07-0.30
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Typical Applications
ASTM A959 S32760
Wrought stainless steel products; recommended composition limits for adoption by product standards (clause 1.1)
ASTM A959 .-
Wrought stainless steel products; recommended composition limits for adoption by product standards (clause 1.1)
Key Differences
Can ASTM A959 S32760 Be Substituted With ASTM A959 .-?
ASTM A959 S32760 and ASTM A959 .- share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.
On M-EX Right Now
ASTM A959 S32760
0 active listings and RFQs →
ASTM A959 .-
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between ASTM A959 S32760 and ASTM A959 .-?
ASTM A959 S32760 specifies Cu, Mo, W which are not specified for ASTM A959 .-. ASTM A959 .- specifies Cb, Ti which are not specified for ASTM A959 S32760.
Can ASTM A959 S32760 be substituted with ASTM A959 .-?
ASTM A959 S32760 and ASTM A959 .- share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.