ASTM A959:2011 S38400 Steel: Specifications & Listings

ASTM A959:2011 S38400: Austenitic stainless steel grade (UNS S38400) with the composition limits of ASTM A959-11. Carbon up to 0.04% and chromium 15.0-17.0%.

Category: Stainless Steel
Grade Details
GradeASTM A959:2011 S38400
Standard ASTM A959:2011
ApplicationsWrought stainless steel products; recommended composition limits for adoption by product standards (clause 1.1)
Equivalent / Similar Grades
Grade Standard Region Live on M-EX
IS 11169 (Part 2) X02Ni18Cr16 IS 11169 (Part 2):2023 India No activity yet
Grade ComparisonCompare With a Specific Grade →
Grade Standard Match
IS 11169 (Part 2) X02Ni18Cr16 IS 11169 (Part 2):2023 Strong Match
IS 1570 (Part 5) X02Cr19Ni10 IS 1570 (Part 5):1985 Related Material
IS 1570 (Part 7) 3Cr18Ni11H IS 1570 (Part 7):1992 Related Material
IS 11169 (Part 2) X02Cr19Ni10 IS 11169 (Part 2):1989 Related Material
IS 11169 (Part 2) X02Cr19Ni9 IS 11169 (Part 2):2023 Related Material
IS 11169 (Part 2) X02Cr18Ni9Cu3 IS 11169 (Part 2):2023 Related Material
IS 11169 (Part 2) X02Cr18Ni8Cu IS 11169 (Part 2):2023 Related Material
IS 11169 (Part 2) X02Cr19Ni11 IS 11169 (Part 2):2023 Related Material
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Chemical Composition (%)
C Cr Mn Ni P S Si
<=0.04 15.0-17.0 <=2.00 17.0-19.0 <=0.045 <=0.030 <=1.00

More data from ASTM A959:2011

From the standard
Other composition limits from Table 1 and its footnotes
UNS number
S38400
Metallurgical class
Austenitic grade: usually predominantly face-centered cubic, hardenable only by cold working
Type
No type number is printed; the grade is identified by its UNS number only
Values
Maximum unless a range or minimum is shown; where two limits are shown for the same element in one grade the more stringent applies
These are the recommended composition limits of the A959 guide, intended for adoption by standards for stainless steel products; they are not a product specification.
Source: ASTM A959:2011, Table 1 and its footnotes

Active ASTM A959:2011 S38400 Listings on M-EX (For Sale)

+ Create a Listing for this grade

No active ASTM A959:2011 S38400 listings at this time.