ASTM A959:2011 S42035 Steel: Specifications & Listings

ASTM A959:2011 S42035: Ferritic stainless steel grade (UNS S42035) with the composition limits of ASTM A959-11. Carbon up to 0.08% and chromium 13.5-15.5%.

Category: Stainless Steel
Grade Details
GradeASTM A959:2011 S42035
Standard ASTM A959:2011
ApplicationsWrought stainless steel products; recommended composition limits for adoption by product standards (clause 1.1)
Equivalent / Similar Grades
Grade Standard Region Live on M-EX
ASTM A240/A240M S42035 ASTM A240/A240M:2025 USA No activity yet
EN 10088-1 X5CrNiMoTi15-2 EN 10088-1:2014 Europe (CEN) No activity yet
EN 10088-2 X5CrNiMoTi15-2 EN 10088-2:2014 Europe No activity yet
Grade ComparisonCompare With a Specific Grade →
Grade Standard Match
ASTM A240/A240M S42035 ASTM A240/A240M:2025 Strong Match
EN 10088-1 X5CrNiMoTi15-2 EN 10088-1:2014 Strong Match
EN 10088-1 X5CrNiMoTi15-2 EN 10088-1:2023 Strong Match
EN 10088-2 X5CrNiMoTi15-2 EN 10088-2:2014 Strong Match
ASTM A959 S42010 ASTM A959:2011 Close Alternative
ASTM A276/A276M S42010 ASTM A276/A276M:2017 Close Alternative
ASTM A959 632 ASTM A959:2011 Related Material
JIS G4304 SUS434 JIS G4304:2021 Related Material
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Chemical Composition (%)
C Cr Mn Mo Ni P S Si Ti
<=0.08 13.5-15.5 <=1.00 0.20-1.20 1.00-2.50 <=0.045 <=0.030 <=1.00 0.30-0.50

More data from ASTM A959:2011

From the standard
Other composition limits from Table 1 and its footnotes
UNS number
S42035
Metallurgical class
Ferritic grade: body-centered cubic, little or no tempered martensite, hardenable only slightly by cold working
Type
No type number is printed; the grade is identified by its UNS number only
Values
Maximum unless a range or minimum is shown; where two limits are shown for the same element in one grade the more stringent applies
Other elements (as printed)
Ti 0.30-0.50
These are the recommended composition limits of the A959 guide, intended for adoption by standards for stainless steel products; they are not a product specification. As printed: nickel and molybdenum printed as stacked pairs (1.00 over 2.50, 0.20 over 1.20); read as the ranges 1.00-2.50 and 0.20-1.20.
Source: ASTM A959:2011, Table 1 and its footnotes

Active ASTM A959:2011 S42035 Listings on M-EX (For Sale)

+ Create a Listing for this grade

No active ASTM A959:2011 S42035 listings at this time.

Register for Alerts

Buyer RFQs for ASTM A959:2011 S42035

+ Post an RFQ for this grade

No open buyer requirements for ASTM A959:2011 S42035 at this time.

Register for Alerts