Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Chemical Composition (%)
C
Cr
Cu
Mn
Mo
Ni
P
S
Si
0.95-1.10
16.0-18.0
<=0.50
0.30-1.00
0.40-0.65
<=0.75
<=0.025
<=0.025
0.30-1.00
More data from ASTM A959:2011
From the standard
Other composition limitsfrom Table 1 and its footnotes
UNS number
S44025
Metallurgical class
Martensitic grade: can be hardened by heat treating and quenching and then tempered; delivered annealed or hardened and tempered
Type
No type number is printed; the grade is identified by its UNS number only
Values
Maximum unless a range or minimum is shown; where two limits are shown for the same element in one grade the more stringent applies
Other elements (as printed)
Cu 0.50
These are the recommended composition limits of the A959 guide, intended for adoption by standards for stainless steel products; they are not a product specification.