BS 970:1955 EN202 Steel: Specifications & Listings

BS 970:1955 EN202: EN202: Carbon-manganese case-hardening steel (semi-free cutting). Specified in BS 970:1955, Part 2.

Category: Free Machining Steel
Grade Details
GradeBS 970:1955 EN202
Standard BS 970:1955
ApplicationsBars and billets for forging; forgings and drop-forgings; bars for machining; bright bars. For this type in cold drawn condition see En 7A.
Equivalent / Similar Grades
Grade Standard Region Live on M-EX
BS 970 (Part 1) 214M15 BS 970 (Part 1):1983 UK No activity yet
Grade ComparisonCompare With a Specific Grade →
Grade Standard Match
BS 970 (Part 1) 214A15 BS 970 (Part 1):1983 Strong Match
BS 970 (Part 3) 210M15 BS 970 (Part 3):1991 Strong Match
BS 970 (Part 1) 214M15 BS 970 (Part 1):1983 Strong Match
BS 970 (Part 1) 210M15 BS 970 (Part 1):1983 Strong Match
BS 970 (Part 1) 210A15 BS 970 (Part 1):1983 Close Alternative
BS 970 (Part 1) 216M28 BS 970 (Part 1):1983 Close Alternative
BS 970 (Part 1) 220M07 BS 970 (Part 1):1983 Close Alternative
BS 970 (Part 1) 230M07 BS 970 (Part 1):1983 Close Alternative
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Chemical Composition (%)
C Si Mn S P
<=0.18 0.05-0.35 1.20-1.50 0.10-0.18 <=0.050
Mechanical Properties
Tensile Strength ≥587 MPa (38 tons/sq in, converted)
Elongation ≥20%
Condition Core, after heat treatment (lowest-strength condition of the standard)

More data from BS 970:1955

From the standard
Condition of material on delivery
A
Bars and billets for forging as rolled or forged unless order states otherwise.
B
Forgings and drop-forgings as forged unless order states otherwise.
C
Bars for machining as rolled unless order states otherwise.
D
Bright bars cold worked or bright machined unless order states otherwise.
Source: BS 970:1955, Part 2, En 202 (page 187)
Mechanical properties
ConditionRuling section or size (in)Tensile strength (tons/sq in)Yield stress (tons/sq in)Elongation (%)Izod impact (ft lb)Brinell (HB)Proof stress 0.2% (tons/sq in), when requested
Core, after heat treatment-38-2030--
Values as printed in BS 970:1955; tensile strength, yield stress and proof stress in tons/sq in, Izod in ft lb. Minimum unless a range is shown.
Source: BS 970:1955, Part 2, En 202 (page 187)
Heat treatment
Blank carburise (1 1/8 in diameter test bars)
880/930 C
Refine (1 1/8 in diameter test bars)
870/900 C, cool in air, oil or water
Harden (oil or water) (1 1/8 in diameter test bars)
770/790 C
Temperatures in degrees C as printed.
Source: BS 970:1955, Part 2, En 202 (page 187)
Notes
Note
See Appendix A for single quench treatment. By arrangement with the purchaser tests may be carried out on samples from which blank carburising has been omitted or modified to a short heating period.
Source: BS 970:1955, Part 2, En 202
Status in the 1955 edition
Status
Remains in the 1955 edition after Amendment 10
BS 970:1955 was amended up to Amendment 10 (June 1972); steels were moved to the revised Parts 1 to 5 and deleted from this edition.
Source: BS 970:1955, Amendment slips 6 to 10

Active BS 970:1955 EN202 Listings on M-EX (For Sale)

+ Create a Listing for this grade

No active BS 970:1955 EN202 listings at this time.

Register for Alerts

Buyer RFQs for BS 970:1955 EN202

+ Post an RFQ for this grade

No open buyer requirements for BS 970:1955 EN202 at this time.

Register for Alerts