Close Alternative — 79% match
based on chemical composition and mechanical property overlap.
BS 970 EN48 (BS 970:1955) and EN 10089 50CrV4 (EN 10089:2002) are both steel grades.
Both fall under the Spring Steel category.
BS 970 EN48 is typically used for high duty springs, valve springs, while EN 10089 50CrV4 is commonly used for valve springs, high duty coil springs, hand tools.
BS 970 EN48 is defined under British Standards (BS), originating from United Kingdom, while EN 10089 50CrV4 is defined under European Standard (EN), originating from Europe.
As per chemical composition, BS 970 EN48 vs EN 10089 50CrV4 is a 79% match.
Mechanical property data is not available for both grades, so this factor could not be scored.
Combined, this makes them a close alternative overall at 79%.
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property
BS 970 EN48
EN 10089 50CrV4
Tensile Strength
Not specified
1100–1300 MPa
Yield Strength
Not specified
≥1000 MPa
Elongation
Not specified
≥8%
Hardness
Not specified
321–375 HB
Typical Applications
BS 970 EN48
High duty springs, valve springs
EN 10089 50CrV4
Valve springs, high duty coil springs, hand tools
Key Differences
BS 970 EN48 specifies S, P which are not specified for EN 10089 50CrV4.
EN 10089 50CrV4 specifies V which is not specified for BS 970 EN48.
Can BS 970 EN48 Be Substituted With EN 10089 50CrV4?
BS 970 EN48 and EN 10089 50CrV4 are a close alternative rather than a direct substitute. Some properties overlap well, but check the specific chemistry and mechanical rows above against your application's requirements before treating them as interchangeable.
What is the difference between BS 970 EN48 and EN 10089 50CrV4?
BS 970 EN48 specifies S, P which are not specified for EN 10089 50CrV4. EN 10089 50CrV4 specifies V which is not specified for BS 970 EN48.
Can BS 970 EN48 be substituted with EN 10089 50CrV4?
BS 970 EN48 and EN 10089 50CrV4 are a close alternative rather than a direct substitute. Some properties overlap well, but check the specific chemistry and mechanical rows above against your application's requirements before treating them as interchangeable.