Minimal Match — 35% match
based on chemical composition and mechanical property overlap.
BS 970 EN51 (BS 970:1955) and ASTM A959 .- (ASTM A959:2011) are both steel grades.
Both fall under the Stainless Steel category.
BS 970 EN51 is typically used for bars and billets for forging; forgings and drop-forgings; bars for machining; bright bars., while ASTM A959 .- is commonly used for wrought stainless steel products; recommended composition limits for adoption by product standards (clause 1.1).
BS 970 EN51 is defined under British Standards (BS), originating from United Kingdom, while ASTM A959 .- is defined under ASTM International, originating from United States.
As per chemical composition, BS 970 EN51 vs ASTM A959 .- is a 58.1% match.
Mechanical property data is not available for both grades, so this factor could not be scored.
Combined, this makes them a minimal match overall at 35%.
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Typical Applications
BS 970 EN51
Bars and billets for forging; forgings and drop-forgings; bars for machining; bright bars.
ASTM A959 .-
Wrought stainless steel products; recommended composition limits for adoption by product standards (clause 1.1)
Key Differences
ASTM A959 .- specifies Cb, N, Ti which are not specified for BS 970 EN51.
Can BS 970 EN51 Be Substituted With ASTM A959 .-?
BS 970 EN51 and ASTM A959 .- share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.
What is the difference between BS 970 EN51 and ASTM A959 .-?
ASTM A959 .- specifies Cb, N, Ti which are not specified for BS 970 EN51.
Can BS 970 EN51 be substituted with ASTM A959 .-?
BS 970 EN51 and ASTM A959 .- share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.