EN 10025-2 S460JR vs GOST 19281 09G2S

Minimal Match — 35% match based on chemical composition and mechanical property overlap.

EN 10025-2 S460JR (EN 10025-2:2019) and GOST 19281 09G2S (GOST 19281-2014) are both steel grades. Both fall under the Structural Steel category. EN 10025-2 S460JR is typically used for hot rolled products of structural steels, while GOST 19281 09G2S is commonly used for used for bridges, pressure vessels, pipelines, structural frames, and heavy equipment components.. EN 10025-2 S460JR is defined under European Standard (EN) (Europe).

As per chemical composition, EN 10025-2 S460JR vs GOST 19281 09G2S is a 62.2% match. As per mechanical properties, the match is 13%. Combined, this makes them a minimal match overall at 35%.

Frequently Compared With EN 10025-2 S460JR:
CSA G40.21 260W AS/NZS 3679.1 300 CSA G40.21 300W AS/NZS 3679.1 350 CSA G40.21 400W CSA G40.21 480W ASTM A1008 SS Grade 50 ASTM A1008 SS Grade 80 ASTM A572 Gr.65
Other Structural Steel Grades to Compare With EN 10025-2 S460JR:
CSA G40.21 350W CSA G40.21 400A ASTM A283C
Match Breakdown
CHEMISTRY MATCH
62.2%
MECHANICAL MATCH
13%
OVERALL
35%
Specifications
Property EN 10025-2 S460JR GOST 19281 09G2S
Standard EN 10025-2:2019 GOST 19281-2014
Category Structural Steel Structural Steel
C (%) <=0.20 0.07-0.12
Si (%) <=0.55 0.5-0.8
Mn (%) <=1.70 1.3-1.7
P (%) <=0.030 0.035 max
S (%) <=0.030 0.04 max
N (%) <=0.025 Not specified
Cu (%) <=0.55 0.3 max
Nb (%) <=0.05 Not specified
V (%) <=0.13 Not specified
Ti (%) <=0.05 Not specified
Ni (%) Not specified 0.3 max
Cr (%) Not specified 0.3 max
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property EN 10025-2 S460JR GOST 19281 09G2S
Tensile Strength 550-720 MPa 490-640 MPa
Yield Strength >=460 MPa 345 MPa min
Elongation >=17% 21% min
Condition Nominal thickness up to 16 mm (tensile for 3 to 100 mm, elongation for 3 to 40 mm), longitudinal test pieces Not specified
Hardness Not specified 140-190 HB
Typical Applications
EN 10025-2 S460JR
Hot rolled products of structural steels
GOST 19281 09G2S
Used for bridges, pressure vessels, pipelines, structural frames, and heavy equipment components.
Key Differences
Can EN 10025-2 S460JR Be Substituted With GOST 19281 09G2S?
EN 10025-2 S460JR and GOST 19281 09G2S share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.
Forms & Sizes Available on M-EX
EN 10025-2 S460JR
No active listings currently.
GOST 19281 09G2S
Plate → (2 listings)
Thickness: 10–10 mm (0.39–0.39 in)
Width: 1500–1500 mm (59.06–59.06 in)
Length: 2900–3800 mm (114.17–149.61 in)
On M-EX Right Now
EN 10025-2 S460JR
0 active listings and RFQs →
GOST 19281 09G2S
2 active listings and RFQs →
Frequently Asked Questions
What is the difference between EN 10025-2 S460JR and GOST 19281 09G2S?
EN 10025-2 S460JR specifies N, Nb, V, Ti which are not specified for GOST 19281 09G2S. GOST 19281 09G2S specifies Ni, Cr which are not specified for EN 10025-2 S460JR.
Can EN 10025-2 S460JR be substituted with GOST 19281 09G2S?
EN 10025-2 S460JR and GOST 19281 09G2S share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.