EN 10028-3 P460NH vs EN 10028-3 P420NL2

Close Alternative — 70.9% match based on chemical composition and mechanical property overlap.

EN 10028-3 P460NH (EN 10028-3:2017) and EN 10028-3 P420NL2 (EN 10028-3:2017) are both steel grades. Both fall under the Alloy Steel category. EN 10028-3 P460NH is typically used for flat products for pressure equipment, while EN 10028-3 P420NL2 is commonly used for flat products for pressure equipment. EN 10028-3 P460NH is defined under European Standard (EN), originating from Europe, while EN 10028-3 P420NL2 is defined under European Standard (EN), originating from Europe.

As per chemical composition, EN 10028-3 P460NH vs EN 10028-3 P420NL2 is a 95.8% match. As per mechanical properties, the match is 21.1%. Combined, this makes them a close alternative overall at 70.9%.

Frequently Compared With EN 10028-3 P460NH:
IS 4367 07Cr4Mo6 UNI 11234 100Cr6 IS 1570 (Part 7) 10Cr36Mo10H EN 10028-2 10CrMo9-10 IS 1570 (Part 4) 10Mo6 IS 1570 (Part 4) 07Cr4Mo6 NF A35-565 100C6 IS 1570 (Part 4) 103Cr6 IS 1570 (Part 4) 10Cr20Mo6 IS 4367 10Cr9Mo10 IS 1570 (Part 7) 10Mo6H IS 1570 (Part 4) 103Cr4
Match Breakdown
CHEMISTRY MATCH
95.8%
MECHANICAL MATCH
21.1%
OVERALL
70.9%
Specifications
Property EN 10028-3 P460NH EN 10028-3 P420NL2
Standard EN 10028-3:2017 EN 10028-3:2017
Category Alloy Steel Alloy Steel
C (%) <=0.20 <=0.20
Si (%) <=0.60 <=0.60
Mn (%) 1.10-1.70 1.10-1.70
P (%) <=0.025 <=0.020
S (%) <=0.010 <=0.005
Al (%) >=0.020 >=0.020
N (%) <=0.025 <=0.020
Cr (%) <=0.30 <=0.30
Cu (%) <=0.70 <=0.30
Mo (%) <=0.10 <=0.10
Nb (%) <=0.05 <=0.05
Ni (%) <=0.80 <=0.80
Ti (%) <=0.03 <=0.03
V (%) <=0.20 <=0.20
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property EN 10028-3 P460NH EN 10028-3 P420NL2
Tensile Strength 570-730 MPa 540-690 MPa
Yield Strength >=460 MPa >=420 MPa
Elongation >=16% >=19%
Condition Normalized, nominal thickness up to 16 mm Normalized, nominal thickness up to 16 mm
Typical Applications
EN 10028-3 P460NH
Flat products for pressure equipment
EN 10028-3 P420NL2
Flat products for pressure equipment
Can EN 10028-3 P460NH Be Substituted With EN 10028-3 P420NL2?
EN 10028-3 P460NH and EN 10028-3 P420NL2 are a close alternative rather than a direct substitute. Some properties overlap well, but check the specific chemistry and mechanical rows above against your application's requirements before treating them as interchangeable.
On M-EX Right Now
EN 10028-3 P460NH
0 active listings and RFQs →
EN 10028-3 P420NL2
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between EN 10028-3 P460NH and EN 10028-3 P420NL2?
Both grades share a similar composition profile; see the specification table above for the exact chemistry and mechanical property values.
Can EN 10028-3 P460NH be substituted with EN 10028-3 P420NL2?
EN 10028-3 P460NH and EN 10028-3 P420NL2 are a close alternative rather than a direct substitute. Some properties overlap well, but check the specific chemistry and mechanical rows above against your application's requirements before treating them as interchangeable.