EN 10084 15NiCr13 (EN 10084:2008) and IS 1570 (Part 4) 105Cr5 (IS 1570 (Part 4):1988) are both steel grades.
Both fall under the Alloy Steel category.
EN 10084 15NiCr13 is defined under European Standard (EN), originating from Europe, while IS 1570 (Part 4) 105Cr5 is defined under Bureau of Indian Standards (IS), originating from India.
As per chemical composition, EN 10084 15NiCr13 vs IS 1570 (Part 4) 105Cr5 is a 68.4% match.
Mechanical property data is not available for both grades, so this factor could not be scored.
Combined, this makes them a minimal match overall at 35%.
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property
EN 10084 15NiCr13
IS 1570 (Part 4) 105Cr5
Condition
Soft annealed
Not specified
Hardenability
+H band at 1.5 mm from the quenched end: 41 to 48 HRC
Not specified
Hardness
Soft annealed: 229 HB max
Not specified
Typical Applications
EN 10084 15NiCr13
Heavily loaded gears, cams, camshafts
IS 1570 (Part 4) 105Cr5
Not documented
Key Differences
EN 10084 15NiCr13 specifies Ni, P, S which are not specified for IS 1570 (Part 4) 105Cr5.
Can EN 10084 15NiCr13 Be Substituted With IS 1570 (Part 4) 105Cr5?
EN 10084 15NiCr13 and IS 1570 (Part 4) 105Cr5 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.
What is the difference between EN 10084 15NiCr13 and IS 1570 (Part 4) 105Cr5?
EN 10084 15NiCr13 specifies Ni, P, S which are not specified for IS 1570 (Part 4) 105Cr5.
Can EN 10084 15NiCr13 be substituted with IS 1570 (Part 4) 105Cr5?
EN 10084 15NiCr13 and IS 1570 (Part 4) 105Cr5 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.