EN 10084 20MnCr5 vs IS 4432 20Mn5Cr5-S

Strong Match — 95.5% match based on chemical composition and mechanical property overlap.

EN 10084 20MnCr5 (EN 10084:2008) and IS 4432 20Mn5Cr5-S (IS 4432:1988) are both steel grades. Both fall under the Alloy Steel category. EN 10084 20MnCr5 is typically used for gears, shafts, cams, case hardened parts, while IS 4432 20Mn5Cr5-S is commonly used for forgings and fabrication of case-hardened machine or automobile parts. EN 10084 20MnCr5 is defined under European Standard (EN), originating from Europe, while IS 4432 20Mn5Cr5-S is defined under Bureau of Indian Standards (IS), originating from India.

As per chemical composition, EN 10084 20MnCr5 vs IS 4432 20Mn5Cr5-S is a 93.3% match. As per mechanical properties, the match is 100%. Combined, this makes them a strong match overall at 95.5%.

Frequently Compared With EN 10084 20MnCr5:
NF A35-565 100C6 UNI 11234 100Cr6 GB/T 3077 12Cr2Ni4A GOST 4543 12HN3A IS 1570 (Part 4) 10Cr20Mo6 IS 1570 (Part 4) 103Cr4 IS 1570 (Part 4) 103Cr6 IS 1570 (Part 7) 10Cr36Mo10H IS 4367 10Cr9Mo10 IS 4367 07Cr4Mo6 IS 1570 (Part 4) 07Cr4Mo6 IS 1570 (Part 4) 105Cr5
Match Breakdown
CHEMISTRY MATCH
93.3%
MECHANICAL MATCH
100%
OVERALL
95.5%
Specifications
Property EN 10084 20MnCr5 IS 4432 20Mn5Cr5-S
Standard EN 10084:2008 IS 4432:1988
Category Alloy Steel Alloy Steel
C (%) 0.17-0.22 0.17-0.22
Cr (%) 1.00-1.30 1.00-1.30
Mn (%) 1.10-1.40 1.00-1.40
P (%) <=0.025 <=0.035
S (%) <=0.035 0.020-0.035
Si (%) <=0.40 0.15-0.35
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property EN 10084 20MnCr5 IS 4432 20Mn5Cr5-S
Condition Soft annealed Not specified
Hardenability +H band at 1.5 mm from the quenched end: 41 to 49 HRC Not specified
Hardness Soft annealed: 217 HB max Not specified
Core Tensile Strength Not specified 1000-1300 MPa (16 mm) / 1000-1300 MPa (30 mm) / 800-1100 MPa (63 mm)
Core Yield Strength Not specified >=750 MPa (16 mm) / >=700 MPa (30 mm) / >=550 MPa (63 mm)
Core Elongation Not specified >=7% (16 mm) / >=8% (30 mm) / >=10% (63 mm)
Core Reduction of Area Not specified >=25% (16 mm) / >=30% (30 mm) / >=35% (63 mm)
Hardness, annealed (A) Not specified <=217 HB
Typical Applications
EN 10084 20MnCr5
Gears, shafts, cams, case hardened parts
IS 4432 20Mn5Cr5-S
Forgings and fabrication of case-hardened machine or automobile parts
Can EN 10084 20MnCr5 Be Substituted With IS 4432 20Mn5Cr5-S?
EN 10084 20MnCr5 and IS 4432 20Mn5Cr5-S overlap closely enough on chemistry and mechanical properties that IS 4432 20Mn5Cr5-S is often considered as a substitute for EN 10084 20MnCr5 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.
Forms & Sizes Available on M-EX
EN 10084 20MnCr5
Round Bar → (22 listings)
Diameter: 50–75 mm (1.97–2.95 in)
Length: 4700–6900 mm (185.04–271.65 in)
IS 4432 20Mn5Cr5-S
No active listings currently.
On M-EX Right Now
EN 10084 20MnCr5
22 active listings and RFQs →
IS 4432 20Mn5Cr5-S
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between EN 10084 20MnCr5 and IS 4432 20Mn5Cr5-S?
Both grades share a similar composition profile; see the specification table above for the exact chemistry and mechanical property values.
Can EN 10084 20MnCr5 be substituted with IS 4432 20Mn5Cr5-S?
EN 10084 20MnCr5 and IS 4432 20Mn5Cr5-S overlap closely enough on chemistry and mechanical properties that IS 4432 20Mn5Cr5-S is often considered as a substitute for EN 10084 20MnCr5 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.