EN 10088-1 1.4401 vs EN 10088-1 X2CrNiMo17-12-2

Close Alternative — 78.6% match based on chemical composition and mechanical property overlap.

EN 10088-1 1.4401 (EN 10088-1:2014) and EN 10088-1 X2CrNiMo17-12-2 (EN 10088-1:2014) are both steel grades. Both fall under the Stainless Steel category. EN 10088-1 1.4401 is defined under European Standard (EN), originating from Europe, while EN 10088-1 X2CrNiMo17-12-2 is defined under European Standard (EN), originating from Europe.

As per chemical composition, EN 10088-1 1.4401 vs EN 10088-1 X2CrNiMo17-12-2 is a 78.6% match. Mechanical property data is not available for both grades, so this factor could not be scored. Combined, this makes them a close alternative overall at 78.6%.

Frequently Compared With EN 10088-1 1.4401:
EN 10088-1 1.4845 EN 10088-1 1.4301 GB/T 3280 06Cr19Ni10 GOST 5632 08X18H10 GOST 5632 12Kh13 GOST 5632 06Kh23N28 EN 10088-1 1.4006 IS 1570 (Part 7) 11Cr17Ni13W3TiH IS 1570 (Part 7) 12Cr12MoVH IS 1570 (Part 7) 12Cr13H IS 1570 (Part 7) 20Cr12MoNiVH ASTM A959 201L
Match Breakdown
CHEMISTRY MATCH
78.6%
MECHANICAL MATCH
No shared data
OVERALL
78.6%
Specifications
Property EN 10088-1 1.4401 EN 10088-1 X2CrNiMo17-12-2
Standard EN 10088-1:2014 EN 10088-1:2014
Category Stainless Steel Stainless Steel
C (%) ≤0.07 <=0.030
Si (%) ≤1.00 <=1.00
Mn (%) ≤2.00 <=2.00
Cr (%) 16.5–18.5 16.5-18.5
Ni (%) 10.5–13.5 10.0-13.0
Mo (%) 2.0–2.5 2.00-2.50
P (%) Not specified <=0.045
S (%) Not specified <=0.015
N (%) Not specified <=0.10
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property EN 10088-1 1.4401 EN 10088-1 X2CrNiMo17-12-2
Tensile Strength ≥520 MPa Not specified
Yield Strength ≥210 MPa Not specified
Elongation ≥40% Not specified
Hardness ≤215 HB Not specified
Typical Applications
EN 10088-1 1.4401
Marine, chemical processing, pharmaceutical equipment
EN 10088-1 X2CrNiMo17-12-2
Not documented
Key Differences
Can EN 10088-1 1.4401 Be Substituted With EN 10088-1 X2CrNiMo17-12-2?
EN 10088-1 1.4401 and EN 10088-1 X2CrNiMo17-12-2 are a close alternative rather than a direct substitute. Some properties overlap well, but check the specific chemistry and mechanical rows above against your application's requirements before treating them as interchangeable.
Forms & Sizes Available on M-EX
EN 10088-1 1.4401
Sheet → (4 listings)
Thickness: 6–6 mm (0.24–0.24 in)
Width: 1250–1250 mm (49.21–49.21 in)
Length: 2500–3400 mm (98.43–133.86 in)
EN 10088-1 X2CrNiMo17-12-2
No active listings currently.
On M-EX Right Now
EN 10088-1 1.4401
4 active listings and RFQs →
EN 10088-1 X2CrNiMo17-12-2
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between EN 10088-1 1.4401 and EN 10088-1 X2CrNiMo17-12-2?
EN 10088-1 X2CrNiMo17-12-2 specifies P, S, N which are not specified for EN 10088-1 1.4401.
Can EN 10088-1 1.4401 be substituted with EN 10088-1 X2CrNiMo17-12-2?
EN 10088-1 1.4401 and EN 10088-1 X2CrNiMo17-12-2 are a close alternative rather than a direct substitute. Some properties overlap well, but check the specific chemistry and mechanical rows above against your application's requirements before treating them as interchangeable.