EN 10088-1 X11CrMoWVNb9-1-1 vs EN 10028-2 X10CrMoVNb9-1

Related Material — 65% match based on chemical composition and mechanical property overlap.

EN 10088-1 X11CrMoWVNb9-1-1 (EN 10088-1:2014) and EN 10028-2 X10CrMoVNb9-1 (EN 10028-2:2017) are both steel grades. EN 10088-1 X11CrMoWVNb9-1-1 is classified under Stainless Steel, while EN 10028-2 X10CrMoVNb9-1 is classified under Alloy Steel — a different category, which is worth noting alongside the chemistry match below. EN 10088-1 X11CrMoWVNb9-1-1 is defined under European Standard (EN), originating from Europe, while EN 10028-2 X10CrMoVNb9-1 is defined under European Standard (EN), originating from Europe.

As per chemical composition, EN 10088-1 X11CrMoWVNb9-1-1 vs EN 10028-2 X10CrMoVNb9-1 is a 67.3% match. Mechanical property data is not available for both grades, so this factor could not be scored. Combined, this makes them a related material overall at 65%.

Frequently Compared With EN 10088-1 X11CrMoWVNb9-1-1:
EN 10088-1 1.4845 ASTM A959 .- GOST 5632 06Kh23N28 EN 10088-1 1.4006 EN 10088-1 1.4301 EN 10088-1 1.4401 GB/T 3280 06Cr19Ni10 GOST 5632 08X18H10 IS 1570 (Part 7) 11Cr17Ni13W3TiH IS 1570 (Part 7) 12Cr12MoH IS 1570 (Part 7) 12Cr12MoVH IS 1570 (Part 7) 12Cr12Ni2Mo
Match Breakdown
CHEMISTRY MATCH
67.3%
MECHANICAL MATCH
No shared data
OVERALL
65%
Specifications
Property EN 10088-1 X11CrMoWVNb9-1-1 EN 10028-2 X10CrMoVNb9-1
Standard EN 10088-1:2014 EN 10028-2:2017
Category Stainless Steel Alloy Steel
C (%) 0.09-0.13 0.08-0.12
Si (%) 0.10-0.50 <=0.50
Mn (%) 0.30-0.60 0.30-0.60
P (%) <=0.020 <=0.020
S (%) <=0.010 <=0.005
Cr (%) 8.5-9.5 8.00-9.50
Mo (%) 0.90-1.10 0.85-1.05
Ni (%) 0.10-0.40 <=0.30
N (%) 0.050-0.090 0.030-0.070
Al (%) <=0.040 <=0.040
Nb (%) 0.060-0.10 0.06-0.10
V (%) 0.18-0.25 0.18-0.25
W (%) 0.90-1.10 Not specified
B (%) 0.0005-0.0050 Not specified
Cu (%) Not specified <=0.30
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property EN 10088-1 X11CrMoWVNb9-1-1 EN 10028-2 X10CrMoVNb9-1
Tensile Strength Not specified 580-760 MPa
Yield Strength Not specified >=445 MPa
Elongation Not specified >=18%
Condition Not specified Usual delivery condition normalized and tempered (+NT), nominal thickness up to 60 mm; transverse direction, Yield Strength is ReH, Elongation is A
Typical Applications
EN 10088-1 X11CrMoWVNb9-1-1
Not documented
EN 10028-2 X10CrMoVNb9-1
Flat products for pressure purposes
Key Differences
Can EN 10088-1 X11CrMoWVNb9-1-1 Be Substituted With EN 10028-2 X10CrMoVNb9-1?
EN 10088-1 X11CrMoWVNb9-1-1 and EN 10028-2 X10CrMoVNb9-1 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.
On M-EX Right Now
EN 10088-1 X11CrMoWVNb9-1-1
0 active listings and RFQs →
EN 10028-2 X10CrMoVNb9-1
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between EN 10088-1 X11CrMoWVNb9-1-1 and EN 10028-2 X10CrMoVNb9-1?
Different category: EN 10088-1 X11CrMoWVNb9-1-1 is Stainless Steel, EN 10028-2 X10CrMoVNb9-1 is Alloy Steel. EN 10088-1 X11CrMoWVNb9-1-1 specifies W, B which are not specified for EN 10028-2 X10CrMoVNb9-1. EN 10028-2 X10CrMoVNb9-1 specifies Cu which is not specified for EN 10088-1 X11CrMoWVNb9-1-1.
Can EN 10088-1 X11CrMoWVNb9-1-1 be substituted with EN 10028-2 X10CrMoVNb9-1?
EN 10088-1 X11CrMoWVNb9-1-1 and EN 10028-2 X10CrMoVNb9-1 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.