EN 10088-1 X1CrNi25-21 vs IS 6603 X01Cr25Ni21

Strong Match — 100% match based on chemical composition and mechanical property overlap.

EN 10088-1 X1CrNi25-21 (EN 10088-1:2014) and IS 6603 X01Cr25Ni21 (IS 6603:2024) are both steel grades. Both fall under the Stainless Steel category. EN 10088-1 X1CrNi25-21 is defined under European Standard (EN), originating from Europe, while IS 6603 X01Cr25Ni21 is defined under Bureau of Indian Standards (IS), originating from India.

As per chemical composition, EN 10088-1 X1CrNi25-21 vs IS 6603 X01Cr25Ni21 is a 100% match. Mechanical property data is not available for both grades, so this factor could not be scored. Combined, this makes them a strong match overall at 100%.

Frequently Compared With EN 10088-1 X1CrNi25-21:
EN 10088-1 1.4845 IS 1570 (Part 7) 11Cr17Ni13W3TiH IS 1570 (Part 7) 12Cr12Ni2Mo GOST 5632 08X18H10 EN 10088-1 1.4006 EN 10088-1 1.4301 EN 10088-1 1.4401 IS 1570 (Part 7) 12Cr12MoH ASTM A959 .- GB/T 3280 06Cr19Ni10 GOST 5632 06Kh23N28 IS 1570 (Part 7) 12Cr12MoVH
Match Breakdown
CHEMISTRY MATCH
100%
MECHANICAL MATCH
No shared data
OVERALL
100%
Specifications
Property EN 10088-1 X1CrNi25-21 IS 6603 X01Cr25Ni21
Standard EN 10088-1:2014 IS 6603:2024
Category Stainless Steel Stainless Steel
C (%) <=0.020 <=0.020
Si (%) <=0.25 <=0.25
Mn (%) <=2.00 <=2.00
P (%) <=0.025 <=0.025
S (%) <=0.010 <=0.010
Cr (%) 24.0-26.0 24.0-26.0
Mo (%) <=0.20 <=0.20
Ni (%) 20.0-22.0 20.0-22.0
N (%) <=0.10 <=0.10
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property EN 10088-1 X1CrNi25-21 IS 6603 X01Cr25Ni21
Tensile Strength Not specified 470-670 MPa
Condition Not specified Solution annealed, conditions 1C, 1E, 1D, 1X, 1G and 2D, rod only; Yield Strength is Rp0.2, Elongation is A (longitudinal)
Typical Applications
EN 10088-1 X1CrNi25-21
Not documented
IS 6603 X01Cr25Ni21
General purposes, semi-finished products, bars, wire rods and bright bars
Can EN 10088-1 X1CrNi25-21 Be Substituted With IS 6603 X01Cr25Ni21?
EN 10088-1 X1CrNi25-21 and IS 6603 X01Cr25Ni21 overlap closely enough on chemistry and mechanical properties that IS 6603 X01Cr25Ni21 is often considered as a substitute for EN 10088-1 X1CrNi25-21 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.
On M-EX Right Now
EN 10088-1 X1CrNi25-21
0 active listings and RFQs →
IS 6603 X01Cr25Ni21
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between EN 10088-1 X1CrNi25-21 and IS 6603 X01Cr25Ni21?
Both grades share a similar composition profile; see the specification table above for the exact chemistry and mechanical property values.
Can EN 10088-1 X1CrNi25-21 be substituted with IS 6603 X01Cr25Ni21?
EN 10088-1 X1CrNi25-21 and IS 6603 X01Cr25Ni21 overlap closely enough on chemistry and mechanical properties that IS 6603 X01Cr25Ni21 is often considered as a substitute for EN 10088-1 X1CrNi25-21 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.