EN 10088-1 X1CrNiMoAlTi12-11-2 vs EN 10088-1 1.4301

Minimal Match — 35% match based on chemical composition and mechanical property overlap.

EN 10088-1 X1CrNiMoAlTi12-11-2 (EN 10088-1:2023) and EN 10088-1 1.4301 (EN 10088-1:2014) are both steel grades. Both fall under the Stainless Steel category. EN 10088-1 X1CrNiMoAlTi12-11-2 is defined under European Standard (EN), originating from Europe, while EN 10088-1 1.4301 is defined under European Standard (EN), originating from Europe.

As per chemical composition, EN 10088-1 X1CrNiMoAlTi12-11-2 vs EN 10088-1 1.4301 is a 46.9% match. Mechanical property data is not available for both grades, so this factor could not be scored. Combined, this makes them a minimal match overall at 35%.

Frequently Compared With EN 10088-1 X1CrNiMoAlTi12-11-2:
GB/T 3280 06Cr19Ni10 ASTM A959 .- GOST 5632 08X18H10 EN 10088-1 1.4401 EN 10088-1 1.4845 IS 1570 (Part 7) 11Cr17Ni13W3TiH IS 1570 (Part 7) 12Cr12MoH IS 1570 (Part 7) 12Cr12Ni2Mo GOST 5632 06Kh23N28 EN 10088-1 1.4006 IS 1570 (Part 7) 12Cr12MoVH IS 1570 (Part 7) 12Cr13H
Match Breakdown
CHEMISTRY MATCH
46.9%
MECHANICAL MATCH
No shared data
OVERALL
35%
Specifications
Property EN 10088-1 X1CrNiMoAlTi12-11-2 EN 10088-1 1.4301
Standard EN 10088-1:2023 EN 10088-1:2014
Category Stainless Steel Stainless Steel
C (%) <=0.015 ≤0.07
Si (%) <=0.10 ≤1.00
Mn (%) <=0.10 ≤2.00
P (%) <=0.010 ≤0.045
S (%) <=0.005 ≤0.030
Cr (%) 11.0-12.5 17.5–19.5
Mo (%) 1.75-2.25 Not specified
Ni (%) 10.2-11.3 8.0–10.5
Al (%) 1.35-1.75 Not specified
Ti (%) 0.20-0.50 Not specified
N (%) <=0.010 Not specified
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property EN 10088-1 X1CrNiMoAlTi12-11-2 EN 10088-1 1.4301
Tensile Strength Not specified ≥520 MPa
Yield Strength Not specified ≥210 MPa
Elongation Not specified ≥45%
Hardness Not specified ≤215 HB
Typical Applications
EN 10088-1 X1CrNiMoAlTi12-11-2
Not documented
EN 10088-1 1.4301
Food equipment, chemical vessels, architectural, kitchenware
Key Differences
Can EN 10088-1 X1CrNiMoAlTi12-11-2 Be Substituted With EN 10088-1 1.4301?
EN 10088-1 X1CrNiMoAlTi12-11-2 and EN 10088-1 1.4301 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.
Forms & Sizes Available on M-EX
EN 10088-1 X1CrNiMoAlTi12-11-2
No active listings currently.
EN 10088-1 1.4301
Sheet → (3 listings)
Thickness: 6–6 mm (0.24–0.24 in)
Width: 1250–1250 mm (49.21–49.21 in)
Length: 2500–3300 mm (98.43–129.92 in)
On M-EX Right Now
EN 10088-1 X1CrNiMoAlTi12-11-2
0 active listings and RFQs →
EN 10088-1 1.4301
3 active listings and RFQs →
Frequently Asked Questions
What is the difference between EN 10088-1 X1CrNiMoAlTi12-11-2 and EN 10088-1 1.4301?
EN 10088-1 X1CrNiMoAlTi12-11-2 specifies Mo, Al, Ti, N which are not specified for EN 10088-1 1.4301.
Can EN 10088-1 X1CrNiMoAlTi12-11-2 be substituted with EN 10088-1 1.4301?
EN 10088-1 X1CrNiMoAlTi12-11-2 and EN 10088-1 1.4301 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.