EN 10088-1 X5CrNiMo17-12-2 vs EN 10088-1 X6CrNiMoNb17-12-2
Strong Match — 93.8% match
based on chemical composition and mechanical property overlap.
EN 10088-1 X5CrNiMo17-12-2 (EN 10088-1:2014) and EN 10088-1 X6CrNiMoNb17-12-2 (EN 10088-1:2023) are both steel grades.
Both fall under the Stainless Steel category.
EN 10088-1 X5CrNiMo17-12-2 is defined under European Standard (EN), originating from Europe, while EN 10088-1 X6CrNiMoNb17-12-2 is defined under European Standard (EN), originating from Europe.
As per chemical composition, EN 10088-1 X5CrNiMo17-12-2 vs EN 10088-1 X6CrNiMoNb17-12-2 is a 93.8% match.
Mechanical property data is not available for both grades, so this factor could not be scored.
Combined, this makes them a strong match overall at 93.8%.
Frequently Compared With EN 10088-1 X5CrNiMo17-12-2:
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Typical Applications
EN 10088-1 X5CrNiMo17-12-2
Marine, chemical, pharmaceutical equipment
EN 10088-1 X6CrNiMoNb17-12-2
Not documented
Key Differences
EN 10088-1 X5CrNiMo17-12-2 specifies N which is not specified for EN 10088-1 X6CrNiMoNb17-12-2.
Can EN 10088-1 X5CrNiMo17-12-2 Be Substituted With EN 10088-1 X6CrNiMoNb17-12-2?
EN 10088-1 X5CrNiMo17-12-2 and EN 10088-1 X6CrNiMoNb17-12-2 overlap closely enough on chemistry and mechanical properties that EN 10088-1 X6CrNiMoNb17-12-2 is often considered as a substitute for EN 10088-1 X5CrNiMo17-12-2 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.
What is the difference between EN 10088-1 X5CrNiMo17-12-2 and EN 10088-1 X6CrNiMoNb17-12-2?
EN 10088-1 X5CrNiMo17-12-2 specifies N which is not specified for EN 10088-1 X6CrNiMoNb17-12-2.
Can EN 10088-1 X5CrNiMo17-12-2 be substituted with EN 10088-1 X6CrNiMoNb17-12-2?
EN 10088-1 X5CrNiMo17-12-2 and EN 10088-1 X6CrNiMoNb17-12-2 overlap closely enough on chemistry and mechanical properties that EN 10088-1 X6CrNiMoNb17-12-2 is often considered as a substitute for EN 10088-1 X5CrNiMo17-12-2 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.