Related Material — 66% match
based on chemical composition and mechanical property overlap.
GB/T 3077 12Cr2Ni4A (GB/T 3077-2015) and SAE J404 50B46 (SAE J404:2009) are both steel grades.
Both fall under the Alloy Steel category.
GB/T 3077 12Cr2Ni4A is typically used for used for gears, shafts, pinions, aircraft parts, heavy-duty bearings, and transmission components., while SAE J404 50B46 is commonly used for chemistry-only alloy steel grade; see the composition notes for product scope.
GB/T 3077 12Cr2Ni4A is defined under Guobiao Standards (GB/T), originating from China, while SAE J404 50B46 is defined under SAE International, originating from United States.
As per chemical composition, GB/T 3077 12Cr2Ni4A vs SAE J404 50B46 is a 66% match.
Mechanical property data is not available for both grades, so this factor could not be scored.
Combined, this makes them a related material overall at 66%.
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property
GB/T 3077 12Cr2Ni4A
SAE J404 50B46
Tensile Strength
980-1180 MPa
Not specified
Yield Strength
785-980 MPa
Not specified
Elongation
10-14%
Not specified
Hardness
58-62 HRC (case)
Not specified
Typical Applications
GB/T 3077 12Cr2Ni4A
Used for gears, shafts, pinions, aircraft parts, heavy-duty bearings, and transmission components.
SAE J404 50B46
Chemistry-only alloy steel grade; see the composition notes for product scope
Can GB/T 3077 12Cr2Ni4A Be Substituted With SAE J404 50B46?
GB/T 3077 12Cr2Ni4A and SAE J404 50B46 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.
What is the difference between GB/T 3077 12Cr2Ni4A and SAE J404 50B46?
Both grades share a similar composition profile; see the specification table above for the exact chemistry and mechanical property values.
Can GB/T 3077 12Cr2Ni4A be substituted with SAE J404 50B46?
GB/T 3077 12Cr2Ni4A and SAE J404 50B46 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.