Strong Match — 86.8% match
based on chemical composition and mechanical property overlap.
IS 1570 (Part 5) X66Cr13 (IS 1570 (Part 5):1985) and EN 10088-1 X65Cr13 (EN 10088-1:2023) are both steel grades.
Both fall under the Stainless Steel category.
IS 1570 (Part 5) X66Cr13 is defined under Bureau of Indian Standards (IS), originating from India, while EN 10088-1 X65Cr13 is defined under European Standard (EN), originating from Europe.
As per chemical composition, IS 1570 (Part 5) X66Cr13 vs EN 10088-1 X65Cr13 is a 86.8% match.
Mechanical property data is not available for both grades, so this factor could not be scored.
Combined, this makes them a strong match overall at 86.8%.
Frequently Compared With IS 1570 (Part 5) X66Cr13:
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Key Differences
EN 10088-1 X65Cr13 specifies P, S which are not specified for IS 1570 (Part 5) X66Cr13.
Can IS 1570 (Part 5) X66Cr13 Be Substituted With EN 10088-1 X65Cr13?
IS 1570 (Part 5) X66Cr13 and EN 10088-1 X65Cr13 overlap closely enough on chemistry and mechanical properties that EN 10088-1 X65Cr13 is often considered as a substitute for IS 1570 (Part 5) X66Cr13 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.
What is the difference between IS 1570 (Part 5) X66Cr13 and EN 10088-1 X65Cr13?
EN 10088-1 X65Cr13 specifies P, S which are not specified for IS 1570 (Part 5) X66Cr13.
Can IS 1570 (Part 5) X66Cr13 be substituted with EN 10088-1 X65Cr13?
IS 1570 (Part 5) X66Cr13 and EN 10088-1 X65Cr13 overlap closely enough on chemistry and mechanical properties that EN 10088-1 X65Cr13 is often considered as a substitute for IS 1570 (Part 5) X66Cr13 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.